DXL Group QUALITY ASSURANCE TEST MANUAL February 2020 Version 5

DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

  • Upload
    others

  • View
    4

  • Download
    0

Embed Size (px)

Citation preview

Page 1: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

DXL Group QUALITY ASSURANCE TEST

MANUAL February 2020 Version 5

Page 2: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 2 of 72 February 2020 Version 5

DXL Group

QUALITY ASSURANCE TEST MANUAL

TABLE OF CONTENTS

SUMMARY ------------------------------------------------------------------------------------------------------------------- 3

DXL GROUP POLICY STATEMENT --------------------------------------------------------------------------------------- 3

TESTING PROCEDURES ---------------------------------------------------------------------------------------------------- 4

SAMPLE SUBMISSION GUIDELINE -------------------------------------------------------------------------------------- 9

VENDOR CONFIRMATION FORM ------------------------------------------------------------------------------------- 11

PROTOCOL INDEX -------------------------------------------------------------------------------------------------------- 12

Page 3: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 3 of 72 February 2020 Version 5

SUMMARY OF THE DXL GROUP TESTING PROGRAM

This DXL Group Quality Assurance Test Manual provides the administrative procedures and quality assurance requirements under the testing program. The Consumer Products Services Division of Bureau Veritas (BVCPS) is the approved laboratory under this program and will perform testing on all items as requested by DXL Group and its suppliers as outlined in this manual. DXL Group performance standards are based on past experience. The Performance Standards are used as a guideline for the evaluation of DXL Group acceptability. Most test methods and test procedures are originated from:

ASTM (American Society of Testing and Materials) AATCC (American Association of Textile Chemists and Colorists) CPSC (Consumer Product Safety Commission) FTC (Federal Trade Commission)

REGULATORY COMPLIANCE NOTICE

In addition, all products or product components sold to DXL Group, must meet the provisions of all U.S. Federal, State and Local Regulations as well as International restricted substance regulations. These include, but are not limited to:

Code of Federal Regulations - Standard for the Flammability of Clothing Textiles

FTC Trade Regulation Rule for Care Labeling of Textile Wearing Apparel

FTC Rules and Regulations under the Textile Fiber, Wool and Fur Products Identification Act

State Regulations for the Feather and Down Products Industry

CPSC Rules and Regulations

U.S. State & Federal, and International Regulations for Restricted Substances

California Proposition 65 Fabric Mills, Garment Factories and Trim Suppliers must provide a continuing guarantee of compliance “free of harmful substances” with the inclusion of a valid OEKO-TEX certificate or provide test results assuring to meet U.S. and International regulations.

DXL Group POLICY STATEMENT

1. DXL Group is committed to delivering quality merchandise to the DXL Group customer.

2. This program is based on the mandate that all merchandise purchased by DXL Group must be tested to meet all applicable laws and regulatory requirements, in addition to ensuring compliance with DXL Group customer satisfaction and acceptability.

3. DXL Group accepts test reports from BVCPS or a BVCPS affiliate. Any exceptions must be agreed to in advance with DXL Group.

4. This testing or any subsequent result does not limit DXL Group rights or diminish or remove vendor or manufacturer's responsibilities and obligations under the Purchase Order Terms and Conditions.

Page 4: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 4 of 72 February 2020 Version 5

TESTING PROCEDURES

I. DXL GROUP RESPONSIBILITY

Provide the vendor access to the DXL Group Quality Assurance Test Manual/Test Protocols/TRF/FRI forms/Fabric Inspection forms, etc. and all other Vendor Compliance Requirements.

http://www.destinationxl.com/media/content/vendors/

When a product fails testing, DXL Group will determine the disposition as to retest or cancellation of the order, etc.

II. VENDOR RESPONSIBILITY

IMPORTANT NOTICES FOR VENDORS

THE SUBMITTER OF FABRIC, TRIM/COMPONENT, ETC. TESTING MUST INCLUDE THE ASSOCIATED MILL/SUPPLIER OEKO-TEX CERTIFICATE WITH EACH BV SUBMISSION, OTHERWISE, THE SUBMITTER IS RESPONSIBLE TO PAY THE COST FOR THE CHEMICAL TESTS CONDUCTED DUE TO THE LACK OF THE CERTIFICATE.

THE TRF MUST BE ACCURATELY COMPLETED AND A COPY INCLUDED WITH EACH SUBMISSION. IF THE INCORRECT TESTS ARE REQUESTED ON THE TRF, THE VENDOR WILL BE RESPONSIBLE TO PAY THE COST FOR THE TESTS.

HOW TO SUBMIT SAMPLES TO BV FOR TESTING

Retrieve and complete the most current DXL Group trf located through the following link http://www.destinationxl.com/media/content/vendors/ OR complete the BV ECOMMERCE DXL Group trf (online test request form) by accessing BV BOOKINGS module through BVOneSource. Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. How to complete the trf, see page 10. Contact [email protected] for all testing questions.

Fabric/Accessories Testing Submission: If the same fabric quality (same weight, construction and finish) is used in multiple styles and is ordered in multiple colors, only one color requires a full test package while all remaining additional colors require the additional color test package. Do not request a full test for multiple colors of the same quality. If additional colors are submitted to BV at a later date, list the full fabric test report # on the trf, and check the Additional Color Only box so that BV only conducts the additional color test. The listed full fabric test report must be within the fabric tests validity period of 6 months. See pages 5-10 for additional details.

Trim/Components Testing Submission: If the same component/trim quality (same material, construction, weight, etc.) is used in multiple styles and is ordered in multiple colors, only one color requires a full test package while all remaining additional colors require the additional color test package. Do not request a full test for multiple colors of the same quality. If additional colors are submitted to BV at a later date, reference the full test report # on the trf, and check the Additional Color Only box so that BV only conducts the additional color test. The listed full test report must be within the trim/component validity period of 12 months. See pages 5-10 for additional details.

Page 5: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 5 of 72 February 2020 Version 5

Garment Testing Submission: Garment testing is required on one color only for each style, and must be conducted on the production garments. The production garments should also include all required sewn-on and heat transfer labels when submitting to BV for testing. The garment test trf should include all fabric, trim, label, etc. previous test report #’s that are associated with the finished garment style. Ensure the listed previous test reports are within the item’s validity period. See pages 5-10 for additional details.

TESTING AND TESTING TIMELINES

Click on the below link to access the DXL Group Quality Assurance Test Manual, Test Protocols, TRF, FRI and Fabric Inspection process requirements/forms, and all other Vendor Compliance Requirements.

http://www.destinationxl.com/media/content/vendors/

All initial or first tests will be paid by the DXL Group; applicable to Global Sourcing Direct vendors only. All retest invoices are the responsibility of the Vendor.

As a vendor to DXL Group, you are fully responsible for all fabric, garment, trim/component, labels (locally sourced) and special claims testing of production merchandise. All must pass or be approved by the DXL Group QA team before production and shipment can occur. The best timing for fabric and trim/component testing is after the bulk submissions have been approved by the DXL Group and within at least 45-60 days of the xfactory date. The best timing for garment testing is after the PP/TOP samples have been approved by the DXL Group and within at least 30-45 days of the xfactory date.

Fabric testing timeline is required every 6 months for each style/color/fabrication, and/or when changes have been made in production or the supplier has changed.

Trim/Component/Elastic/Label testing timeline is required every 12 months for each garment trim/component/label and/or when changes have been made in production or the supplier has changed.

Garment testing timeline is required every 6 months for each style/fabrication in one color only.

Belts/Suspenders/Metal Accessories/Neck Ties testing timeline is required every 12 months.

The timelines are applicable to all DXL Group brands/styles including Core and E3 Replenishment Programs. Analytical Testing - OEKO-TEX certificate: Analytical (chemical) testing determines if harmful chemicals are present in DXL Group products; and ensures compliance with U.S. and International regulations. An OEKO-TEX certificate verifies an item is certified free of harmful chemicals and is safe for human use. Regarding testing, an OEKO-TEX certificate will exempt most chemical tests, therefore, all vendors/suppliers of DXL Group fabrics, trim/components, logos, labels, etc. must provide DXL Group a copy of each associated OEKO-TEX certificate and must also include a copy with each test submission to BV. If the certificate is not provided to BV, the submitter will be responsible for the cost of the chemical tests. Nickel Leaching: Any metal trim/component in direct contact to the skin which results in a positive nickel spot

test will require a full Nickel Leaching test at the expense of the vendor.

Page 6: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 6 of 72 February 2020 Version 5

AZO Dye Colorants: DXL Group requires that all products are AZO Free or within the AZO Dye Colorant maximum requirement of <30mg/kg.

Formaldehyde Content: DXL Group requires that all products in direct contact with the skin are within the formaldehyde content maximum requirement of 75 mg/kg.

Lead Testing: Any applicable surface coating or substrate lead test result must not exceed the maximum allowable limits.

California Proposition 65: All products will be reviewed against the requirements of California Proposition 65 to determine testing applicability.

Heavy Metals content in packaging materials per Model Toxics in Packaging Legislation per the Toxics in Packaging Clearinghouse (TPCH) requirements. All packaging materials must pass the TPCH requirements. Vendors must provide evidence of compliance in the form of a certificate from an accredited testing laboratory for any locally sourced packaging. This test will be at the expense of the vendor.

Fabric Testing: All fabrics used in DXL Group products must be tested per the appropriate protocol and meet DXL Group standard test requirements. The supplier’s OEKO-TEX certificate must be provided to DXL Group and included with every BV submission. Bulk production cannot proceed without DXL Group review and approval. Fabric testing is required every 6 months for each style/color/fabrication, and/or when changes have been made in production or the supplier has changed. Full fabric test is only required on one color of the same fabrication. All other colors of the same fabrication should be tested for “Additional Color” test only.

Development Stage: Newly developed fabrics must go through our specification and quality testing to verify the proper fabric properties, finishes and performance.

Production Fabric Stage: Production fabric testing must be conducted on approved bulk fabric of the correct construction, color, finish, etc. All bulk fabric testing should be completed and approved prior to bulk ex-mill. Bulk fabric testing should be planned accordingly and test results received within at least 45-60 days from x-mill date so not to delay bulk garment cutting and sewing. The final test report will help determine/verify the care instructions and fiber content labeling for the garment. Bulk fabric must not be cut until written approval is issued by DXL Group.

Fabric used in Color-Blocked Garments: Fabrics must be in the form of a color blocked mock-up and tested for colorfastness per the care instructions and colorfastness to water to ensure self-staining does not occur.

Fabrics containing Wicking and/or Anti-fade finishes: the fabric mill must try to submit every color in one submission to Bureau Veritas for testing. Example: If your order for style KT-1000 includes 20 colors, all 20 colors should be sent together on one trf for testing, if possible.

Fabric produced for Garment Wash programs: The fabric mill must send the garment factory two (2) square yards of all colors or the entire shipment if produced in a timely fashion, so the factory can perform the garment wash process. Once the garment wash process is complete, the garment factory will be responsible to send the fabric in all colors to Bureau Veritas for fabric testing. The fabric mill should advise the factory as to what testing package is required, such as fabric test, additional color test and/or any special claims.

Page 7: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 7 of 72 February 2020 Version 5

Trim/Component Testing: ALL trims/components used on DXL Group products must be tested separately per their respective protocol. The supplier’s OEKO-TEX certificate must be provided to DXL Group and BV. Trim testing should be planned accordingly and test results received within at least 45-60 days from x-factory date so not to delay bulk garment cutting and sewing. Bulk production cannot proceed without DXL Group review and approval. Trim/Component testing is required every 12 months, and/or when changes have been made in production or the supplier has changed. Full trim test is only required on one color of the same fabrication. All other colors of the same fabrication should be tested for “Additional Color” test only. YKK Brand products are EXEMPT from testing.

Zippers: DXL Group preferred supplier is YKK. Vendor local manufacturing brands will be accepted based on a passing test report from Bureau Veritas and the supplier’s OEKO-TEX certificate.

Shank Buttons: DXL Group preferred supplier is Scovil. However, vendor local manufacturing brands will be accepted based on a passing test report from Bureau Veritas and the supplier’s OEKO-TEX certificate.

Non-Breakable Buttons for the Dress Shirt Program: Dress shirt buttons must pass the non-breakable button test as well as all other applicable button tests. See button protocol for test requirements.

Knit/Mesh Lining Insert Trim Fabric (Jacket Relaxer) used for Sport Coats and Suit Jackets: conduct colorfastness to crocking and perspiration only. See requirements in the trim/component protocol.

A new protocol, 808 Rib Cuffs /Collars /Bottom Hems /Bottom Bands, was added to Version 5 of the manual.

Garment Testing: Is carried out to ensure the fabric, components/trims and garment construction are compatible and meet DXL Group quality performance standard requirements. The garment test assesses and verifies the garment performance, labeling and restricted substance conformance. Bulk production cannot proceed without DXL Group review and approval. Garment testing is required every 6 months for each style/fabrication in one color only.

Full garment testing is required on one color of each style using both approved bulk fabric and trims. However, if a garment is color-blocked, a full garment test is required on one color combination and colorfastness only for each additional color combination.

All production styles have to be garment tested as soon as bulk fabric, trims/components and labels become available to factory. Garment Testing should be completed at a minimum of 30-45 days prior to x-factory. At times, we may require garment testing during the sampling stage to verify its performance and functionality.

Sweater Testing: Full testing for sweaters must be conducted on complete garments. Knit-down panels can be used for additional color testing.

The vendor is responsible to notify labs regarding appropriate protocol, and all special claims as applicable in the garment stage, to ensure that proper testing is performed according to DXL Group requirements. If the garment contains a belt, Protocol 805 must be conducted.

Durable Press testing for wrinkle resistant/non-iron/easy care claims is conducted in both the fabric and garment test packages. All other claims testing are required on the fabric only, unless otherwise instructed.

Repeat styles require testing every 6 months if produced by the same factory unless agreed upon by DXL Group Quality Assurance. Any change of fabric mill, factory, supplier, trim, component, label, etc. before the 6 month period will require immediate full testing.

Page 8: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 8 of 72 February 2020 Version 5

The additional performance tests for the Premium Pants is included in the new protocol 809 Premium Pants - Additional Performance Tests, page 68.

Care/Fiber Content Booklet and Heat Transfer Label (HTL): the layout with the correct wording must be submitted to the QA team [email protected] for approval before placing the final order with your supplier. Packaging Materials Testing (polybags, ink, inserts, stickers, etc.): All packaging materials must be tested for Heavy Metals content per Model Toxics in Packaging Legislation/ Toxics in Packaging Clearinghouse (TPCH) requirements. All packaging materials (polybags, ink, inserts, stickers, etc.) must pass the TPCH requirements. Vendors must provide evidence of compliance in the form of a certificate or test report confirming compliance; from both nominated and locally sourced packaging suppliers. Labels/Logo Stamp Testing: Garment Sewn-On Labels/Heat Transfer Labels/Size Labels/Care Booklets/Brand Labels/Logo Prints or Stamps/Etc., must pass DXL Group requirements per protocol 800. Testing is required every 12 months, and/or when changes have been made in production or the supplier has changed. For heat transfer labels or any stamps printed directly onto the garment fabric, the durability wash test (one color only) must be tested on the correct fabric quality. All label suppliers or vendors must ensure testing per DXL Group label protocol is conducted either internally or at a BV location. The supplier’s OEKO-TEX certificate must be provided to DXL Group and BV, if available. Testing is required initially, after testing report has expired and when changes in production are made or the supplier has changed. DXL Group reserves the right to reject any shipment if the testing program was not followed or test results were not accepted by DXL Group.

Page 9: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 9 of 72 February 2020 Version 5

III. BVCPS RESPONSIBILITY

SAMPLE SUBMISSION GUIDELINE

Sample submission to BVCPS: Fabric Testing: A minimum of two (2) square yards must be submitted for full testing in one (1) colorway along with a minimum of one (1) square yard fabric in each additional colorway. Fabric must be identical in every aspect to bulk production piece goods. If an OEKO-TEX certificate is received from the mill/supplier with a submission, all applicable chemical tests should be exempted and a remark added to the report regarding the exemption. Trim/Component Testing: All trims/components used on DXL Group products must be tested separately per their respective protocol. See Trim/Component testing protocols for test requirements. If an OEKO-TEX certificate is received from the mill/supplier with a submission, all applicable chemical tests should be exempted and a remark added to the report regarding the exemption.

Components/Findings Functional/Decorative Trim

Number of Samples Required

Zippers 6 Zippers

Buttons, Snaps, etc. 10 Samples (If tested in garment stage)

Elastic 3 Yards/Samples

Applied Trim: Lace, Bows, Ribbon, Patches, Etc. 8 Samples, 1 Yard OR 4 Garments

Screen print, Embroidery / Appliqué 5 Samples OR 4 Garments

Garment Testing: Send four (4) garments in each style in the largest size available for complete garment testing. Include test report #’s on the trf for all garment style associated trims/components, etc. If trims/components, etc. have not been previously tested, send sufficient garments or loose trim/components, etc. to also conduct the component testing. Best case scenario, all garment component testing should be completed before the garment test. Garments must be made on production machinery and must represent bulk production.

A completed DXL Group Test Request Form (TRF) must be submitted with garments/components/fabric, etc. BVCPS will not accept a sample if the form is incomplete. The Vendor may obtain a Test Request Form (TRF) through the DXL Group link http://www.destinationxl.com/media/content/vendors/ OR complete the BV ECOMMERCE DXL Group trf (online test request form) by accessing BV BOOKINGS module through BVOneSource.

Garments must include all bulk trim/components, accessories and embellishments. If additional garments, fabric and/or trim/components are required, BVCPS will immediately contact the vendor

and copy the DXL Group QA team at [email protected].

VISUALLY UNSATISFACTORY SAMPLES (stains, tears, and missing pieces) WILL NOT BE ACCEPTED FOR TESTING!

Retests: All retests are the vendor’s responsibility.

Note: For product retests, the previous test report number must be referenced on the Test Request Form (trf) along with a list of the tests requiring a retest. If a previous report number is not referenced, the full fabric, component and/or garment tests may be performed on the submission at the vendor’s expense. All retested fees are the vendor’s responsibility.

When the Test Request Form is incomplete, the laboratory will notify the originating vendor and copy the DXL Group QA team at [email protected]. Until proper information is received, testing will be delayed.

Page 10: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 10 of 72 February 2020 Version 5

Complete testing and evaluate the test results (See DXL Group Standard Test Package). Rate the product by:

o Pass ―The product provides good overall consumer serviceability and requires no improvement.

o Fail ―The product has deficiencies of such severity that the customer dissatisfaction will likely result and / or noncompliance or regulatory requirements. The product cannot be sold until improvements are made.

Include pictures of the tested product, trf and OEKO-TEX certificate in the report.

Include pictures of the garment labels and failures in the report. Reports will be emailed to DXL Group and submitter as well as posted on BVOS.

Click on the below icon for instructions on how to complete the trf.

HOW TO COMPLETE

THE TRF Sample Preparation Guidelines:

Collect production quality sample

Each sample must fulfill the minimum sample size requirement

Fill out the Test Request Form completely

Send Test Application to Testing Lab Laboratory Test Turnaround Time:

Regular: 5 working days after receipt of sample

Express: Within 3 working days after receipt of sample at surcharge of 40%

Nest Business Day: Next working day are available for some tests at surcharge of 100% Some test standards require specified testing period, default service turnaround time may not be applicable, no express and emergency services provided.

Testing Working Day Calculation:

Sample arrived laboratory Sample log-in Service level available

From 9:00 am to 11:00 am Same day morning Emergency service Express service Regular service

From 11:00 am to 15:00 pm Same day afternoon Regular service

After 15:00 pm Next working day Emergency service Express service Regular service

Test Sample Receipt & Hold Memo

Test Sample Receipt provides information of test selected and expected report available date for regarding test submission. Hold Memo indicates testing halt when encountering situation of insufficient / inadequate information or samples.

Report Distribution To: Applicant (Test Submitter) Cc: Per Test Request From

Test report copy will be sent to Client by email when completed.

Third Party Billing Official confirmation from Invoice recipient is required

Page 11: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 11 of 72 February 2020 Version 5

VENDOR CONFIRMATION FORM OF DXL GROUP QUALITY STANDARDS

I acknowledge receipt of DXL Group Quality Assurance Test Manual. I have read and understand the policies and procedures set forth and agree to comply with them. Company Name (Type or Print) Company Officer’s Signature (Type or Print Name Signed Above)

Title Date

Page 12: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 12 of 72 February 2020 Version 5

Protocol Index Protocol Name Page

100F Woven Fabric (Tops & Bottoms) 13 100G Woven Garment (Tops & Bottoms) 15 100.5F Pocketing & Waistband Curtain Fabric 16 101F Woven Denim Fabric 17 101G Denim Garment 19 200F Knit Fabric 21 200G Knit Garment 23 201F Loungewear / Underwear / Terry Robe / Sleepwear Fabric 24 201G Loungewear / Underwear / Terry Robe / Sleepwear Garment 26 202F Swim Fabric 27 202G Swimwear 29 300F&G Sweaters 30 400F Leather & Suede Hides 32 400G Leather & Suede Garments 33 500F Lining Fabric (Applies to all Textile Items) 34 600G Hats & Caps 36 601G Socks & Hosiery 38 602G Neck Ties 40 700 F Outerwear Fabric (Shell Only) 41 700G Outerwear Garment (With or Without Lining) 43 701F Sports Coats / Jackets, Suits Fabric (Shell Only) 44 701G Sports Coats / Jackets, Suits – Garment (With or Without Lining) 46 800 Trims/Components Buttons, Shank Buttons, Snaps/Rivets, Zippers, Hook & Eye, Other Hardware

47

801 Elastic 53 802 Special Claims 54 803 Belts 57 804 Suspenders 60 805 Belts (sold together with a garment) 62 806 Accessories (Scarves, Neck Warmers, Gloves, Handkerchiefs, Earmuffs) 807 Rain Poncho 808 Rib Cuffs /Collars /Bottom Hems /Bottom Bands 809 Premium Pants - Performance Tests Zipper Requirements

63 65 67 68 69

Page 13: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 13 of 72 February 2020 Version 5

100F Woven Fabric (Tops & Bottoms) Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight ASTM D3776 -5%/+10% from claim

Fabric Count ASTM D3775 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

100% Cotton, Linen, or Rayon: -4% All others: -3% Growth: +1%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade 4.0 No adverse effects

Skew/Torque AATCC 179

Method 1, Option 1 3% maximum

Tensile Strength ASTM D5034

<2.4 oz/yd2: 20 lbs.min. 2.5-4.0 oz/yd2: 25 lbs. min. 4.1-6.0 oz/yd2: 30 lbs. min. 6.1-7.9 oz/yd2: 40 lbs. min ≥8.0 oz/yd2: 55 x 40 lbs. min

Tear Strength ASTM D1424

<2.4 oz/yd2: 1.5 lbs.min. 2.5-4.0 oz/yd2: 2.5 x 2.0 lbs. min. 4.1-6.0 oz/yd2: 2.5 lbs. min. > 6.1-7.9 oz/yd2: 3.0 lbs. min. >8.0 oz/yd2: 4.0 lbs. min.

Seam Slippage ASTM D1683 20 lbs.min @ ¼”

*Stretch & Recovery ASTM D3107

≥ 5% Spandex (test in stretch direction only) Recovery: 85% minimum Growth: 5% maximum ( Measure after 30 minutes)

Page 14: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 14 of 72 February 2020 Version 5

100F Woven Fabric (Tops & Bottoms) Page 2 of 2

TEST CITATION / METHOD CRITERIA

Performance (continued)

*Abrasion Resistance (Twill pant fabric only)

ASTM D3886

Stretch Twill: 100 cycles min Unwashed: ≤8.0 oz/yd2: 300 cycles min >8.0 oz/yd2: 500 cycles min Washed: ≤8.0 oz/yd2: 100 cycles min >8.0 oz/yd2: 200 cycles min Note: Observe every 20 cycles

*Pile retention (corduroy only)

ASTM D4685 Abrasive Wheel: CS10, Head Weight:250 g Grade 3 Face Minimum after 300 cycles Grade 4 Back Minimum after 100 cycles

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.5 @ 20 AFU

CF to Water AATCC 107

Color block / Contrast trims only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 15: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 15 of 72 February 2020 Version 5

100G Woven Garment (Tops & Bottoms) Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label RN# or WPL # Country of Origin Care Label Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

100% Cotton, Linen, Rayon: -4% All others: -3%, Growth: +1%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0, Color Change: Grade4.0 Self-Staining: Grade4.5

Seam Skew/Torque AATCC / ASTM TS-004 3% maximum

Seam Strength** ASTM D1683

< 6.0 oz/yd2: Shirt: 20 lbs. min. / Pant: 25 lbs. min. 6.0-7.9 oz/yd2: Shirt: 25 lbs. min. / Pant: 30 lbs. min. ≥8.0 oz/yd2: 35 lbs. min Lining: 20 lbs.

Seam Slippage** ASTM D1683 20 lbs.min @ ¼”

Component Attachment Strength/ Zipper Strength Properties

Refer to protocol 800 for actual requirement Note: Shanks must be tested for Attachment and Tension

Component Functionality Function as Intended

Pocket Stress Area ASTM D1683 mod Bottoms: 15 lbs. min. Tops: 10 lbs. min.

Notes: 1. Any components not previously tested are required to test to appropriate standard. 2. Please refer to special claims protocol as applicable. **Seam Strength/Slippage: test the following seams: Tops: Side, Shoulder, Center Back, Yoke, Armhole, Sleeve, Collar Bottoms: Side, Inseam, Seat, Back Rise, Crotch, Zipper stress area

Page 16: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 16 of 72 February 2020 Version 5

100.5F Pocketing, Binding Trim, Piping Trim & Waistband Curtain Fabric Page 1 of 1

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

Fabric Weight ASTM D3776 -5%/+10% from claim

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

Woven: -4% Growth: +1% Knit: -5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

Page 17: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 17 of 72 February 2020 Version 5

101F Woven Denim Fabric Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value (all colors/washes) AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight ASTM D3776 -5%/+10% from claim

Fabric Count ASTM D3775 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

Washed: -3 % Stretch/Rigid: -4% Growth: +1%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Skew/Torque AATCC 179

Method 1, Option 1 3% maximum

Tensile Strength ASTM D5034 8-10 oz/yd2 : 55 x 35 min 10.1-12.0 oz/yd2: 65 x 40 min >12.0 oz/yd2: 85 x 70 min

Tear Strength ASTM D1424 8-10 oz/yd2 : 4.0 x 3.0 min 10.1-12.0 oz/yd2: 4.0 x 3.5 min >12.0 oz/yd2: 6.5 x 4.0 min

Seam Slippage ASTM D1683 20 lbs.min @ ¼”

*Stretch & Recovery ASTM D3107

≥ 5% Spandex (test in stretch direction only) Recovery: 85% minimum Growth: 5% maximum (Measure after 30 minutes)

Abrasion Resistance ASTM D3886 Stretch Denim: 100 cycles min Unwashed: 500 cycles min Washed: 200 cycles min

Page 18: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 18 of 72 February 2020 Version 5

101F Woven Denim Fabric Page 2 of 2

TEST CITATION / METHOD CRITERIA

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Indigo/Black Dry: Grade3.5 Wet: Grade2.0

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.5 @ 20 AFU

CF to Water AATCC 107

Color block/Contrast Trims Only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Ozone AATCC 109 Grade3.5 1 cycle

CF to Burnt Gas Fumes AATCC 23 Grade3.5 1 cycle

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 19: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 19 of 72 February 2020 Version 5

101G Denim Garment Page 1 of 2

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label RN# or WPL # Country of Origin Care Label Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

*Nickel Spot Test (shank & rivet back only) (Applicable to any metal component intended for prolonged skin contact)

PD CR 12471

Negative Conduct in garment stage only if not already tested in component stage. If positive see “Analytical Requirements” protocol

pH value (all colors/washes) AATCC 81 5-9

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Washed: -3 % Rigid/Stretch: -4% Growth: +1%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0 Color Change: Grade4.0 Self-Staining: Grade4.5

Seam Skew/Torque AATCC TS-004 3% maximum

Seam Strength** ASTM D1683 8-10 oz/yd2 : 35 lbs. min 10.1-12.0 oz/yd2: 40 lbs. min >12.0 oz/yd2: 50 lbs. min

Seam Slippage** ASTM D1683 20 lbs.min @ ¼”

Page 20: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 20 of 72 February 2020 Version 5

101G Denim Garment Page 2 of 2

Notes: 1. Any components not previously tested are required to test to appropriate standard. 2. Please refer to special claims protocol as applicable.

**Seam Strength/Slippage: test the following seams: Tops: Side, Shoulder, Center Back, Yoke, Armhole, Sleeve, Collar Bottoms: Side, Inseam, Seat, Back Rise, Crotch, Zipper stress area

Performance (continued)

Component Attachment Strength/ Zipper Strength Properties

Refer to protocol 800 for actual requirement Note: Shanks must be tested for Attachment and Tension

Component Functionality Function as Intended

Pocket Stress Area ASTM D1683 MOD 20 lbs. min.

Colorfastness

CF to Crocking AATCC 8/116 Dry Class 4.0 Wet Class 3.0

Dark Indigo / Black: Dry Class 3.5 Wet Class 2.0

Page 21: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 21 of 72 February 2020 Version 5

200F Knit Fabric Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight ASTM D3776 -5%/+10% from claim

Fabric Count ASTM D3887 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

-5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0 Satisfactory for Double Face Fleece

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Skew/Torque AATCC 179

Method 1, Option 1 5% maximum

Bursting Strength ASTM D3786 <120 gm/m2: 40 psi ≥120 gm/m2: 55 psi

*Pilling (Only if Claimed Double Face Fleece with Anti-Pill Treatment)

ASTM D3512 Satisfactory @ 30 min

*Stretch & Recovery ASTM D2594

≥ 5% Spandex (test both directions) Recovery: 85% minimum Growth: 5% maximum ( Measure both after 60 minutes)

Page 22: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 22 of 72 February 2020 Version 5

200F Knit Fabric Page 2 of 2

TEST CITATION / METHOD CRITERIA

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.5 @ 20 AFU

CF to Water AATCC 107

Color block / Contrast trims only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 23: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 23 of 72 February 2020 Version 5

200G Knit Garment Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label RN# or WPL # Country of Origin Care Label Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

-5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Satisfactory for Double face fleece Pilling: Grade4.0 Color Change: Grade4.0 Self-Staining: Grade4.5

Seam Skew/Torque AATCC TS-004 5% maximum

Seam Stretchability AATCC TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

Component Functionality Function as Intended

Component Attachment Strength/ Zipper Strength Properties

Refer to protocol 800 for actual requirement

Notes: 1. Any components not previously tested are required to test to appropriate standard 2. Please refer to special claims protocol as applicable.

Page 24: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 24 of 72 February 2020 Version 5

201F Loungewear / Underwear / Terry Robe / Sleepwear Fabric Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight ASTM D3776 -5%/+10% from claim

Fabric Count Woven: ASTM D3775

Knit: ASTM D3887 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

Woven: 100%: Cotton: -4% All others: -3% Growth: +1% Knit: -5% Growth: +2%

General Appearance after care (3HL)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Skew/Torque AATCC 179

Method 1, Option 1 Knit:5% maximum Woven: 3% maximum

Seam Slippage (Woven) ASTM D1683 20 lbs. min @ ¼”

Tensile Strength (Woven) ASTM D5034

<2.4 oz/yd2: 20 lbs.min. 2.5-4.0 oz/yd2: 25 lbs.min. 4.1-6.0 oz/yd2: 30 lbs.min > 6.0 oz/yd2: 40 lbs. min.

Tear Strength (Woven) ASTM D1424

<2.4 oz/yd2: 1.5 lbs.min. 2.5-4.0 oz/yd2: 2.5 x 2.0 lbs .min. 4.1-6.0 oz/yd2: 2.5 lbs. min. > 6.1-7.9 oz/yd2:3.0 lbs. min. >8.0 oz/yd2: 4.0 lbs. min.

Bursting Strength (Knit) ASTM D3786 <120 gm/m2: 40 psi ≥120 gm/m2: 55 psi

Page 25: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 25 of 72 February 2020 Version 5

201F Loungewear / Underwear / Terry Robe / Sleepwear Fabric Page 2 of 2

TEST CITATION / METHOD CRITERIA

Performance (continued)

*Stretch & Recovery Woven: ASTM D3107

Knit: ASTM D2594

Knit: ≥ 5% Spandex (test both directions) Recovery: 85% minimum Growth: 5% maximum ( Measure both after 60 minutes) Woven: ≥ 5% Spandex (test in stretch direction only) Recovery: 85% minimum Growth: 5% maximum ( Measure after 30 minutes)

*Absorbency (Terry Robe Only) ASTM D4772 Ultra-absorbency: 75% min Two-sided terry: 65% min One-sided terry: 35% min

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.0 @ 20 AFU

CF to Water AATCC 107

Color block / Contrast trims only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15

Excludes Robe Fabric Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 26: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 26 of 72 February 2020 Version 5

201G Loungewear / Underwear / Terry Robe / Sleepwear Garment Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label RN# or WPL # Country of Origin Care Label Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Woven: 100%: Cotton:-4%, All others:-3%, Growth:+1% Knit: -5%, Growth: +2%

General Appearance after care (3HL)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0 Color Change: Grade 4.0, Self-Staining: Grade 4.5

Seam Skew/Torque AATCC TS-004 Knit:5% maximum, Woven: 3% maximum

Loss of Lint (Terry Robe Only) Visual No Noticeable Loss

Seam Strength** (Woven) ASTM D1683 <6.0 oz/yd2: 20 lbs. min / ≥ 6.0 oz/yd2: 25 lbs. min

Seam Slippage** (Woven) ASTM D1683 20 lbs. min @ ¼”

Seam Stretchability (Knits) AATCC TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

Seam Strength (Knit boxer/briefs only: test seam strength in the vertical direction pulling the waistband from the body fabric)

ASTM D1683 25 lbs. min

Component Attachment Strength/ Zipper Strength Properties

Refer to protocol 800 for actual requirement

Component Functionality Function as Intended

Pocket Stress Area ASTM D1683 mod Functional: 15 lbs.min./ Non-functional:10 lbs. min.

Notes: 1. Any components not previously tested are required to test to appropriate standard. 2. Please refer to special claims protocol as applicable. **Seam Strength/Slippage: test the following seams: Tops: Side, Shoulder, Center Back, Yoke, Armhole, Sleeve, Collar Bottoms: Side, Inseam, Seat, Back Rise, Crotch, Zipper stress area

Page 27: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 27 of 72 February 2020 Version 5

202F Swim Fabric Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight ASTM D3776 -5%/+10% from claim

Fabric Count Woven: ASTM D3775

Knit: ASTM D3887 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

Woven: -4% Growth: +1% Knit: -5% Growth: +2%

General Appearance after care (3HL)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Skew/Torque AATCC 179

Method 1, Option 1 Knit:5% maximum Woven: 3% maximum

Seam Slippage (Woven) ASTM D1683 20 lbs. min @ ¼”

Tensile Strength (Woven) ASTM D5034

<2.4 oz/yd2: 20 lbs.min. 2.5-4.0 oz/yd2: 25 lbs. min. 4.1-6.0 oz/yd2: 30 lbs. min. > 6.0 oz/yd2: 40 lbs. min.

Tear Strength (Woven) ASTM D1424

<2.4 oz/yd2: 1.5 lbs.min. 2.5-4.0 oz/yd2: 2.5 x 2.0 lbs. min. 4.1-6.0 oz/yd2: 2.5 lbs. min. 6.1-7.9 oz/yd2: 3.0 lbs. min. >8.0 oz/yd2: 4.0 lbs. min.

Bursting Strength (Knit) ASTM D3786 <120 gm/m2: 40 psi ≥120 gm/m2: 55 psi

Page 28: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 28 of 72 February 2020 Version 5

202F Swim Fabric Page 2 of 2

TEST CITATION / METHOD CRITERIA

Performance (continued)

*Stretch & Recovery Woven: ASTM D3107

Knit: ASTM D2594

Knit: ≥ 5% Spandex (test both directions) Recovery: 85% minimum Growth: 5% maximum ( Measure both after 60 minutes) Woven: ≥ 5% Spandex (test in stretch direction only) Recovery: 85% minimum Growth: 5% maximum ( Measure after 30 minutes)

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 20 & 40 AFU Pass/Fail based on 40 AFU rating only Grade 3.0 @ 40 AFU

CF to Water AATCC 107 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Sea Water AATCC 106 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Pool water AATCC 162 Color Change: Grade4.0

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 29: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 29 of 72 February 2020 Version 5

202G Swimwear Garments Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label RN# or WPL # Country of Origin Care Label Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Woven: -4% Growth: +1% Knit: -5% Growth: +2%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0 Color Change: Grade4.0 Self-Staining: Grade4.5

Seam Skew/Torque AATCC TS-004 Knit:5% maximum, Woven: 3% maximum

Seam Strength** (Woven) ASTM D1683 <6.0 oz/yd2: 20 lbs. min / ≥ 6.0 oz/yd2: 25 lbs. min

Seam Slippage** (Woven) ASTM D1683 20 lbs. min @ ¼”

Seam Stretchability (Knit) AATCC TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

Component Attachment Strength / Zipper Strength Properties

Refer to protocol 800 for actual requirement

Component Functionality Function as Intended

Pocket Stress Area ASTM D1683 mod Functional: 15 lbs.min./ Non-functional:10 lbs. min.

Notes: 1. Any components not previously tested are required to test to appropriate standard 2. Please refer to special claims protocol as applicable.

**Seam Strength/Slippage: test the following seams: Tops: Side, Shoulder, Center Back, Yoke, Armhole, Sleeve, Collar Bottoms: Side, Inseam, Seat, Back Rise, Crotch, Zipper stress area

Page 30: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 30 of 72 February 2020 Version 5

300F&G Sweaters Page 1 of 2

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label RN# or WPL # Country of Origin Care Label Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber, ± 3% Blends

Weight per dozen ASTM D3887 mod -5%/+10% from claim

Fabric Count ASTM D3887 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

-5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

-2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0, Color Change: Grade4.0 Self-Staining: Grade4.5

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Seam Skew/Torque AATCC TS-004 5% maximum

Bursting Strength ASTM D3786 <120 gm/m2: 40 psi / ≥120 gm/m2: 50 psi

Page 31: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 31 of 72 February 2020 Version 5

300F&G Sweaters

Page 2 of 2

TEST CITATION / METHOD CRITERIA

Performance (continued)

Seam Stretchability AATCC TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

*Stretch & Recovery ASTM D2594 ≥ 5% Spandex (test both directions) Recovery: 85% minimum / Growth: 5% maximum ( Measure both after 60 minutes)

*Pilling Resistance-(Wool & Wool blends only)

ICI Pilling box method BS NE ISO 12945-1

Wool blends Grade3.0 @ 4 hours (14,400 revolutions) Cashmere / Luxury fibers: Grade3.0 @2 hours (7,200 revolutions)

Component Attachment / Zipper Strength Properties

Refer to protocol 800 for actual requirement

Component Functionality Function as Intended

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.5 @ 20 AFU

CF to Water AATCC 107

Color Block / Contrast Trims only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Notes: 1. Any components not previously tested are required to test to appropriate standard

2. Please refer to special claims protocol as applicable.

Page 32: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 32 of 72 February 2020 Version 5

400F Leather & Suede Hides

Page 1 of 1

TEST CITATION / METHOD CRITERIA

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH AATCC 81 5-9

Physical Characteristics

*Fiber Analysis or Skin Identification

AATCC 20/20A 0% Single Fiber ± 3% Blends

Leather Thickness ASTM D1813 report in millimeters ± 5% from claim

Material Weight ASTM D3776 ± 5% from claim

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Professional Leather Clean

Professional Leather Clean

Per Care Instructions

-2% +1% Growth

General Appearance after care Visual

CPSD-SL-31055-MTHD No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Tensile Strength ASTM D5034 40 lbs. min

Tear Strength ASTM D1424 <6.0 oz/yd2: 2.5 lb min 6.0-7.9 oz/yd2: 3.0 lb min ≥8.0 oz/yd2: 4.0 lb min

Colorfastness

CF to Professional Leather Clean Leather Clean-1 cycle Color Change: Grade4.0 Self-Staining: Grade4.5

CF to Crocking of Leather ASTM D5053 Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.5 @ 20 AFU

Note: Please refer to special claims protocol as applicable.

Page 33: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 33 of 72 February 2020 Version 5

400G Leather & Suede Garments

Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Guide for Select Leather & Imitation Leather Products Textile or Wool Fiber Products Identification Act Care Labeling Rule

Visual

Leather Identification Fiber Content Label RN# or WPL # Country of Origin Care Label Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US The sample should be reviewed against the requirements of California Proposition 65 to determine if additional testing or labeling is required.

Formaldehyde Spot Test (Applicable to any product intended for prolonged skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Base fabric only that comes into contact with skin) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Professional Leather Clean

Per Care Instructions -2%, Growth +1% Differential Shrinkage (Shell/Lining): 2%

General Appearance after care Visual

CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0 Color Change: Grade4.0 Self-Staining: Grade4.5

Seam Strength** ASTM D1683 25 lbs. min. Lining 20 lbs. min.

Seam Slippage** ASTM D1683 20 lb min @ ¼”

Component Attachment Strength / Zipper Strength Properties

Refer to protocol 800 for actual requirement

Component Functionality Function as Intended

Pocket Stress Area ASTM D1683 mod Functional: 15 lbs.min./ Non-functional:10 lbs. min.

Notes: 1. Any components not previously tested are required to test to appropriate standard 2. Please refer to special claims protocol as applicable. **Seam Strength/Slippage: test the following seams: Tops: Side, Shoulder, Center Back, Yoke, Armhole, Sleeve, Collar Bottoms: Side, Inseam, Seat, Back Rise, Crotch, Zipper stress area

Page 34: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 34 of 72 February 2020 Version 5

500F Lining Fabric (Applies to all Textile Items) Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight Woven: ASTM D3776

Knit: ASTM D3887 -5%/+10% from claim

Fabric Count Woven: ASTM D3775

Knit: ASTM D3887 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

Woven: 100% Cotton: -4% All others: -3% Growth: +1% Knit: -5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Woven: Shrinkage -2% Growth +1% Knit: Shrinkage -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Seam Slippage (Woven) ASTM D1683 20 lbs. min @ ¼”

Seam Strength (Woven) ASTM D1683 20 lbs. min

Seam Stretchability (Knit) AATCC TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

Tensile Strength (Woven) ASTM D5034

<3.5 oz/yd2: 20 lbs min 3.5-6.0 oz/yd2: 30 lb min 6.1-7.9 oz/yd2: 40 x 30 lb min ≥8.0 oz/yd2: 60 x 50 lb min

Tear Strength (Woven) ASTM D1424

<3.5 oz/yd2: 1.5 lbs min 3.5-6.0 oz/yd2: 2.5 lb min 6.1-7.9 oz/yd2: 3.0 lb min ≥8.0 oz/yd2: 4.0 lb min

Page 35: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 35 of 72 February 2020 Version 5

500F Lining Fabric (Applies for all Textile Items) Page 2 of 2

TEST CITATION / METHOD CRITERIA

Performance (continued)

Bursting Strength (Knit) ASTM D3786 <120 gm/m2: 40 psi ≥120 gm/m2: 55 psi

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

CF to Light AATCC 16, Option 3 Grade 3.0 @ 10 AFU

CF to Water AATCC 107

Color block / Contrast trims only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Sea Water AATCC 106

Swimwear Only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Pool Water AATCC 162 Swimwear Only Color Change: Grade4.0

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 36: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 36 of 72 February 2020 Version 5

600G Hats & Caps Page 1 of 2

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label (exempt-unless labeled or if Wool) RN# or WPL # (only if includes fiber content labeling) Country of Origin Care Label (exempt-if labeled, must comply to the rules)

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis (only if claimed) AATCC 20/20A 0% Single Fiber, ± 3% Blends Hats are exempt unless something is stated about fiber or if contains wool

Fabric Weight ASTM D3776 -5%/+10% from claim

Fabric Count ASTM D3775 -5%/+10% from claim

Fabric Type Visual As Claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Woven: 100% Cotton: -4%, All others: -3%, Growth: +1% Knit: -5%, Growth: +2% Differential Shrinkage (shell/lining): 2%

Dimensional Stability after Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

-2% Growth +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0

Seam Strength ASTM D1683 10 lbs. min

Seam Stretchability AATCC TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

Page 37: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 37 of 72 February 2020 Version 5

600G Hats & Caps Page 2 of 2

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 20 & 40 AFU Pass/Fail based on 40 AFU rating only Grade 3.0 @ 40 AFU

CF to Water AATCC 107

Color block / Contrast trims only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Notes: 1. Any components not previously tested are required to test to appropriate standard. 2. Please refer to special claims protocol as applicable.

TEST CITATION / METHOD CRITERIA

Performance (continued)

Bursting Strength (knit) ASTM D3786 <120 gm/m2: 40 psi ≥120 gm/m2: 55 psi

Component Attachment Strength Pull Test 15 lbs./10 Seconds

Component Functionality Function as Intended

*Resistance To Corrosion (All Metal Components)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails

Page 38: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 38 of 72 February 2020 Version 5

601G Socks & Hosiery Page 1 of 2

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label Care Label Country of Origin RN# or WPL # Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable.

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

Formaldehyde Spot Test

In-house test method / CPSD-AN-00018-

MTHD

Negative If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber, ± 3% Blends

Weight per Dozen Standard Measure 5%/+10% from claim

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Subjective evaluation on all sizes after wash No more than 6% shrinkage & the ability to fit NAHM forms

General Appearance after care (3HL)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0

Abrasion Resistance of Socks (Heel Area)

ASTM D4966 (Mod) Athletic: 400 cycles minimum Casual / Dress: 200 cycles minimum

Fit Properties-After Laundering CPSD-SL-31006-MTHD Sock Stretch: Biaxial stretch: 0.5 lbs. min – 9 lbs. max Cuff Support: 0.25 lbs./in min – 4.25 lbs./in max Cuff: Correspond to maximum heel girth (inches)

*Antibacterial Activity Assessment (If Claimed Anti-

Microbial, Anti-Bacterial, Odor Control) Test ONE Color only

Refer to Protocol 802 Refer to Protocol 802 for actual requirement

*Water wicking test (If claimed

Moisture Management/Wicking, etc.) Test All Colors

AATCC 197 Refer to Protocol 802 for actual requirement

Page 39: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 39 of 72 February 2020 Version 5

601G Socks & Hosiery Page 2of 2

TEST CITATION / METHOD CRITERIA

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Grade 3.0 @ 10 AFU

CF to Water AATCC 107 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Notes: 1. Any components not previously tested are required to test to appropriate standard. 2. Please refer to special claims protocol as applicable.

Page 40: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 40 of 72 February 2020 Version 5

602G Neck Ties/Pocket Squares Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label RN# or WPL # Country of Origin Care Label

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US The sample should be reviewed against the requirements of California Proposition 65 to determine if additional testing or labeling is required.

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber/± 3% Blends

Fabric Type Visual As claimed

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability after Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

-2% Growth +1%

General Appearance after Dry cleaning

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0 Color Change: Grade4.0 Self-Staining: Grade4.5

Component Attachment Refer to protocol 800 for actual requirement

*Soil Release: Oily Stain Method (if claimed Stain Resistant)

AATCC 130 Test Original & After 1 DC Original: Grade 3.5 After 1 DC: Grade 3.0

Colorfastness

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light (Ties only) AATCC 16, Option 3 Grade 4.0 @ 10 AFU

Notes: 1. Any components not previously tested are required to test to appropriate standard 2. Please refer to special claims protocol as applicable

Page 41: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 41 of 72 February 2020 Version 5

700F Outerwear Fabric (Shell Only)

Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight Woven: ASTM D3776

Knit: ASTM D3887 -5%/+10% from claim

Fabric Count Woven: ASTM D3775

Knit: ASTM D3887 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

Woven: 100% Cotton: -4% All others: -3% Growth: +1% Knit: -5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Woven: Shrinkage -2% Growth +1% Knit: Shrinkage -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Skew/Torque AATCC 179

Method 1, Option 1 Knit:5% maximum Woven: 3% maximum

Tensile Strength (Woven) ASTM D5034 <6.0 oz/yd2 : 30 lbs. min 6.1-7.9 oz/yd2: 40 x 30 lbs. min ≥8.0 oz/yd2: 55 x 40 min

Tear Strength (Woven) ASTM D1424 <6.0 oz/yd2 : 2.5 lbs. min 6.1-7.9 oz/yd2: 3.0 lbs. min ≥8.0 oz/yd2: 4.0 min

Seam Slippage (Woven) ASTM D1683 20 lbs.min @ ¼”

Page 42: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 42 of 72 February 2020 Version 5

700F Outerwear Fabric (Shell Only) Page 2 of 2

TEST CITATION / METHOD CRITERIA

Performance (continued)

Bursting Strength (Knit) ASTM D3786 <120 gm/m2: 40 psi ≥120 gm/m2: 55 psi

*Stretch & Recovery ASTM D3107/2594

Knit: ≥ 5% Spandex (test both directions) Recovery: 85% minimum Growth: 5% maximum ( Measure both after 60 minutes) Woven: ≥ 5% Spandex (test in stretch direction only) Recovery: 85% minimum Growth: 5% maximum ( Measure after 30 minutes)

*Pile retention (corduroy only)

ASTM D4685 Abrasive Wheel: CS10, Head Weight:250 g Grade 3 Face Minimum after 300 cycles Grade 4 Back Minimum after 100 cycles

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 20/40 AFU Pass/Fail based on 40 AFU rating only Grade 3.0 @ 40 AFU

CF to Water AATCC 107

Color block / Contrast trims only Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 43: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 43 of 72 February 2020 Version 5

700G Outerwear Garment (With or Without Lining) Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label Care Label Country of Origin RN# or WPL # Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Woven: 100% Cotton: -4%, All others: -3%, Growth: +1% Knit: -5%, Growth: +2% Differential Shrinkage (Shell/lining): 2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage -2% Growth: +1% Differential Shrinkage (Shell/lining): 2%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc., Pilling: Grade4.0, Color Change: Grade4.0, Self-Staining: Grade4.5

Seam Skew/Torque AATCC TS-004 Knit:5% maximum, Woven: 3% maximum

Seam Strength** ASTM D1683 Shell:25 lbs. min., Lining: 20 lbs.

Seam Slippage** ASTM D1683 20 lbs. min. @ ¼”

Seam Stretchability AATCC / ASTM TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

Component Attachment / Zipper Strength Properties

Refer to protocol 800 for actual requirement

Component Functionality Function as Intended

Pocket Stress Area ASTM D1683 mod Functional: 15 lbs. min./ Non-functional:10 lbs. min.

Notes: 1. Any components not previously tested are required to test to appropriate standard. 2. Please refer to special claims protocol as applicable.

**Seam Strength/Slippage: test the following seams: Tops: Side, Shoulder, Center Back, Yoke, Armhole, Sleeve, Collar Bottoms: Side, Inseam, Seat, Back Rise, Crotch, Zipper stress area

Page 44: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 44 of 72 February 2020 Version 5

701F Sport Coats/Suit Jackets/Suits Fabric (Shell Only) Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH value AATCC 81 5-9

Flammability

Flammability Of Clothing Textiles 16 CFR 1610 Class 1 (if not exempt) All Colors

Physical Characteristics

*Fiber Analysis AATCC 20/20A 0% Single Fiber ± 3% Blends

Fabric Weight ASTM D3776 -5%/+10% from claim

Fabric Count ASTM D3775 -5%/+10% from claim

Fabric Type Visual As claimed

Yarn Size ASTM D1059 No Pass/Fail, report actual results only

Defects/Workmanship Visual Report all defects

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

Woven: 100% Cotton: -4% All others: -3% Growth: +1% Knit: -5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Woven: Shrinkage -2% Growth +1% Knit: Shrinkage -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Appearance after Ironing Hand Iron

Per Care Instructions Color Change: Grade4.0 No adverse effects

Skew/Torque AATCC 179

Method 1, Option 1 Knit:5% maximum Woven: 3% maximum

Tensile Strength (Woven) ASTM D5034 <6.0 oz/yd2 : 30lbs. min 6.1-7.9 oz/yd2: 40 x 30 lbs. min ≥8.0 oz/yd2: 55 x 40 min

Tear Strength (Woven) ASTM D1424 <6.0 oz/yd2 : 2.5 lbs. min 6.1-7.9 oz/yd2: 3.0 lbs. min ≥8.0 oz/yd2: 4.0 min

Seam Slippage (Woven) ASTM D1683 20 lbs.min @ ¼”

Bursting Strength ASTM D3786 <120 gm/m2: 40 psi ≥120 gm/m2: 55 psi

*Pile retention (corduroy only)

ASTM D4685 Abrasive Wheel: CS10, Head Weight:250 g Grade 3 Face Minimum after 300 cycles Grade 4 Back Minimum after 100 cycles

Page 45: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 45 of 72 February 2020 Version 5

701F Sport Coats/Suit Jackets/Suits Fabric (Shell Only) Page 2 of 2

TEST CITATION / METHOD CRITERIA

Performance (continued)

*Stretch & Recovery ASTM D3107

Knit: ≥ 5% Spandex (test both directions) Recovery: 85% minimum Growth: 5% maximum ( Measure both after 60 minutes) Woven: ≥ 5% Spandex (test in stretch direction only) Recovery: 85% minimum Growth: 5% maximum ( Measure after 30 minutes)

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

Dark Colors: Dry Grade3.5 Wet Grade2.5

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.5 @ 20 AFU

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Water AATCC 107

Color block / Contrast trims only Color Change: Grade 4.0 Staining: Grade 3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Note: Please refer to special claims protocol as applicable.

Page 46: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 46 of 72 February 2020 Version 5

701G Sport Coats/Suit Jackets/Suits-Garment (With or Without Lining) Page 1 of 1

TEST CITATION / METHOD CRITERIA

Labeling

Textile Fiber Products Identification Act Care Labeling Rule Wool Products Labeling Act

Visual

Fiber Content Label Care Label Country of Origin RN# or WPL # Size

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable. Do Not test heat transfer labels or woven sewn-on labels

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Physical Characteristics

Defects/Workmanship Visual Report all defects/No Sharp Points/Edges

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Woven: 100% Cotton: -4%, All others: -3%, Growth: +1% Knit: -5%, Growth: +2% Differential Shrinkage (Shell/lining): 2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage -2%, Growth: +1% Differential Shrinkage (Shell/lining): 2%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade 4.0 Color Change: Grade 4.0 Self-Staining: Grade 4.5

Seam Skew/Torque AATCC TS-004 Knit:5% maximum Woven: 3% maximum

Seam Strength** ASTM D1683 25 lbs. min. lining 20 lbs.

Seam Slippage** ASTM D1683 20 lbs. min @ ¼”

Seam Stretchability AATCC / ASTM TS-015 <120 gm/m2: 35% and/or 6 lbs. ≥120 gm/m2: 50% and/or 7 lbs.

Component Attachment Strength/ Zipper Strength Properties

Refer to protocol 800 for actual requirement

Component Functionality Function as Intended

Pocket Stress Area ASTM D1683 mod Functional: 15 lbs. min./ Non-functional:10 lbs. min.

Notes: 1. Any components not previously tested are required to test to appropriate standard 2. Please refer to special claims protocol as applicable.

**Seam Strength/Slippage: test the following seams: Tops: Side, Shoulder, Center Back, Yoke, Armhole, Sleeve, and Collar. Bottoms: Side, Inseam, Seat, Back Rise, Crotch, Zipper stress area.

Page 47: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 47 of 72 February 2020 Version 5

800 Trims/Components

(YKK BRAND PRODUCTS ARE EXEMPT FROM TESTING) Page 1 of 6

TEST CITATION / METHOD CRITERIA

Buttons

Effects of Washing / Dry-cleaning Per care label 3 washes or 1 commercial dry clean No chipping, cracking, paint loss No color transfer, No corrosion

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Attachment strength Pull Method 15 lbs.@ 10 seconds

Manufacturing Qualities Visual No sharp points or edges

*Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

*Unbreakable Buttons (required for dress shirts designated by the style prefix of “DS”)

CPSD-SL-31055 / ASTM D5171

CPSD-SL-31055: Evaluate 30 buttons after 5 / 10 / 15 / 20 washes - No chips, cracks or breakage ASTM D5171: Evaluate 30 buttons under 5.5 in-oz impact energy - No chips, cracks or breakage

Knit/Mesh Lining Insert (Jacket Relaxer)-used in Sport Coats and Suit Jackets

CF to Crocking AATCC 8/116 Dry Grade4.0 / Wet Grade3.0

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

Packaging Materials: Polybags/Ink/Inserts/Stickers/Etc. THE VENDOR SHOULD PROVIDE PASSING TEST RESULTS OR A COC (certificate of conformance) FROM THE SUPPLIER

*Heavy Metals Content In Packaging Materials

Model Toxics in Packaging Legislation of the Toxics in Packaging Clearinghouse (TPCH)

The sum of concentration levels of lead, cadmium, mercury and hexavalent chromium in packaging or packaging components shall not exceed 100 mg/kg (100 ppm) by weight. Note: It is the vendor’s responsibility for the conformity of this requirement.

Page 48: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 48 of 72 February 2020 Version 5

800 Trims/Components (YKK BRAND PRODUCTS ARE EXEMPT FROM TESTING)

Page 2 of 6

TEST CITATION / METHOD CRITERIA

Shank Button

Effects of Washing / Dry-cleaning Per care label 3 washes or 1 commercial dry clean No Chipping, cracking, paint loss, No color transfer No corrosion

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Nickel Spot Test (shank back only) (Applicable to any metal component intended for prolonged skin contact only)

PD CR 12471 Negative If positive see “Analytical Requirements” protocol

Shank Tension Strength (the force it takes to detach the top of the shank from the back (nail/tack) of the shank)

ASTM D1683 (mod.)

Min. 80 lbs.

Shank Attachment Strength (the force to pull the shank button from the waistband)

Pull Method (using the Instron)

Straight position: Min. 60 lbs. Slant position @ 60°: Min. 60 lbs. Report actual data until removal or breakage. Specify if shank breaks/shank pulls out of waistband/or if fabric ruptures

Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Manufacturing Qualities Visual No sharp points or edges

Page 49: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 49 of 72 February 2020 Version 5

800 Trims/Components (YKK BRAND PRODUCTS ARE EXEMPT FROM TESTING)

Page 3 of 6

TEST CITATION / METHOD CRITERIA

Snaps/Rivets

Effects of Washing / Dry-cleaning Per care label 3 washes or 1 commercial dry clean No Chipping, cracking, paint loss, No color transfer No corrosion

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Unsnapping Force (Must be tested on garment or attached to a mock-up panel)

CPSD-SL-31045-MTHD Maximum 8 lbs. Fails if the snap is detached from the garment during the test

Holding Strength (Must be tested on garment or attached to a mock-up panel)

ASTM D7142 15 lbs.@ 10 seconds

Manufacturing Qualities Visual No sharp points or edges

*Nickel Spot Test (Applicable to any metal component intended for prolonged skin contact only)

PD CR 12471 Negative If positive see “Analytical Requirements” protocol

Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Page 50: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 50 of 72 February 2020 Version 5

800 Trims/Components (YKK BRAND PRODUCTS ARE EXEMPT FROM TESTING)

Page 4 of 6

TEST CITATION / METHOD CRITERIA

Shirt Collar Button Extender

Attaches to the collar button

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Tension Test ASTM D1683 (mod.) 15 lbs.

Workmanship Visual No major defects

Manufacturing Qualities Visual No sharp points or edges

Loop Extension Must exceed 1/2”

Functionality Shall function as intended

Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog) spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Page 51: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 51 of 72 February 2020 Version 5

800 Trims/Components (YKK BRAND PRODUCTS ARE EXEMPT FROM TESTING)

Page 5 of 6

TEST CITATION / METHOD CRITERIA

Zipper

Effects of Washing / Dry-cleaning Per care label 3 washes or 1 commercial dry clean No Chipping, cracking, paint loss No color transfer, No corrosion

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Zipper Strength

ASTM D2061

Crosswise Strength, Operability (Zip/Unzip ) Slider Lock Holding Strength, Tab Pull Off Strength Top Stop Strength, Bottom Stop Strength See Zipper Requirements

Manufacturing Qualities Visual No sharp points or edges

Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Hook & Eye

Effects of Washing / Dry-cleaning Per care label 3 washes or 1 commercial dry clean No Chipping, cracking, paint loss No color transfer, No corrosion

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Hook and Eye Tension ASTM D1683 (mod.) 30 lbs.

Attachment Strength Pull Method 15 lbs./10 seconds

Manufacturing Qualities Visual No sharp points or edges

Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Page 52: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 52 of 72 February 2020 Version 5

800 Trims/Components (YKK BRAND PRODUCTS ARE EXEMPT FROM TESTING)

Page 6 of 6

TEST CITATION / METHOD CRITERIA

Other Hardware/ Components/ Fabric Trim: Draw cord/Grommets/Cord Stopper/End Caps/Velcro/Eyelets/Buckles/ and Others made of Metal/Plastic/Fabric, Etc.

Effects of Washing / Dry cleaning Per care label 3 washes or 1 commercial dry clean No Chipping, cracking, paint loss, distortion, No color transfer, No corrosion

Attachment strength Pull Method 15 lbs./10 seconds

Manufacturing Qualities Visual No sharp points or edges

*CF to Crocking (fabric) AATCC 8/116 Dry Grade4.0 / Wet Grade3.0

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

*Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

LABELS/ETC: Garment Sewn-On Labels /Heat Transfer Labels/Size Labels/Care Booklets/Brand Labels/Logo Prints or Stamps/Printed Labels, Heat Seal Tape, Etc.

THE VENDOR SHOULD PROVIDE THE SUPPLIER’S OEKO-TEX CERTIFICATE

*Tagless/Labels -Durability Wash Test

CPSD-SL-31055-MTHD Per care label

Prints/Stamps/HTL, etc. Evaluate and record comments after 10 and 20 wash/dry cycles or 5 dry clean cycles Color Change: Grade 4.0, Self-Staining: Grade 4.5 Appearance: No cracking, peeling, distortion, color transfer, etc. Text must be legible

*CF to Crocking AATCC 8/116 Dry Grade4.0 / Wet Grade3.0

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Page 53: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 53 of 72 February 2020 Version 5

801 Elastic Page 1 of 1

TEST CITATION / METHOD CRITERIA

Analytical

pH Value AATCC 81 5-9

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (as applicable per Adult item)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable per Adult item)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Physical Characteristics

Elastic Width (mm) Standard Measure As claimed

Elastic Weight ASTM D3776 Report actual data

Elastic Construction ASTM D37775 Report actual data Number of Elastic Yarns Visual Report actual data Wrapped Yarns Visual Report actual data Construction/workmanship Visual No Major defects

Performance

Dimensional Stability-Home Laundering (3 washes)

Per Care Instructions Woven: -4% Knit: -6% +1% growth

Dimensional Stability-Dry-cleaning (1 cycle)

Per Care Instructions Shrinkage: -2% No growth

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Pilling: Grade4.0

Stretch Power & Recovery CPSD-SL-31031-MTHD Recovery: 85% minimum Record tension at 20, 40, 60 and 80% elongation

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0, Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0, Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0/Wet Grade3.0

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

*Phenolic Yellowing ISO 105-X18 Solid White or Ivory (test if >50% of surface area) Grade3.5

Page 54: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 54 of 72 February 2020 Version 5

802 Special Claims Page 1 of 3

TEST CITATION / METHOD CRITERIA

*Absorbency AATCC 79 Test Original only on Terry Robes Maximum 30 seconds

*Air Permeability ASTM D737 Windproof Claim Test Original & after 3 HL or 1 DC (per care label) 10 cfm maximum

*Antibacterial/Antimicrobial Activity Test ONE Color only

AATCC 100 or ASTM E2149

If Claimed Anti-Microbial, Anti-Bacterial, Odor Control Test Original & After 10/20 HL Test using Staphylococcus Aureus bacteria only ≥95% Reduction

*Anti-Fade (All Colors) see page 66 for Premium Pants requirement

CPSD-SL-31055-MTHD If Claimed Evaluate after 5 / 10 washes Color Change: Grade 4.0 minimum

*Anti-pill CPSD-SL-31055-MTHD If Claimed Evaluate after 5 / 10 / 15 / 20 washes Pilling: Grade4.0 minimum

*Drying Rate BV Method 50% minimum at 30 minutes

*Feather & down: Content Analysis

ASTM D4524-86 (2005 / IDFB 3

Original As specified (for labeling follow the USA (ADA) Textile Labeling Guidelines for Feather & Down) 2-3% tolerance

*Feather and down: Fill Power IDFB 10-B Original Steam conditioning If no claim is made report value only If claimed(min): + or - 5%

*Feather and down: Turbidity IDFB 11-A Original 300 mm minimum US measurement Hypoallergenic/Super Clean Claim: 500 mm minimum

*Feather and down: oxygen number

IDFB 21/IDFB 7 JIS 6.6

EN 1162

Original Less than 10 Hypoallergenic/Super Clean Claim: Less than 5

*Feather and down: odor IDFL Original No putrid odor

*Feather and down: fat and oil IDFB 4 Original 0.7% min – 2.0% max

*Feather and down: down proof FTM 191-A Method 5530 (mod)

Original Grade 4 min

Page 55: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 55 of 72 February 2020 Version 5

802 Special Claims Page 2 of 3

TEST CITATION / METHOD CRITERIA

* Flocking Durability CPSD-SL-31055-MTHD Per Care instructions

Rate after 3 washes No obvious defects/observations affecting the end performance / appearance, color change, staining, satisfactory performance of the components and trims

*Heat Seal Tape Trim Durability (Before conducting the durability test, the factory must get accurate transfer application specifications from the supplier and then submit to BV or at the supplier location)

CPSD-SL-31055-MTHD Per Care instructions

Wash or dry clean according to proposed care method. Evaluate and record comments after 5 and 10 wash/dry cycles or 5 dry clean cycles No de-lamination, cracking, bubbling, wrinkling, curling, etc. No other adverse effects to the end product or obvious defects in appearance, color change, staining, etc.

*Non Roll Collar CPSD-SL-31055-MTHD If Claimed or Requested Evaluate after 5 / 10 / 15 / 20 washes Collar retains without rolling defect

*Oil Repellency AATCC 118 Stain Proof Claim Test Original & after 5 HL or 1 DC (per care label) Original: minimum 6/ After 5 washes/1DC: minimum 4

*Size Strip Sticker/Sock Band Evaluation

CPSD-31026 Humidity Chamber set at

140 degrees F (60C) at 95% humidity for 48

hours under 10 lbs. of pressure

After the testing period, visually evaluate the sticker and fabric for the following:

The amount of fiber/print removed from the product and remains on the sticker

Any product damage noted

Amount of adhesive residue remaining on the product

Sticker impression remaining on the fabric

Color change on fabric: Grade 4

Sticker de-bonding, curling or degradation

Any other adverse effects

*Soil Release: Oily Stain Method

AATCC 130

If Claimed Stain Resistant Test Original & after 5 HL or 1 DC (per care label) Original: Grade 3.5 After 5 washes/1DC: Grade 3.0

*Tagless/Labels -Durability Wash Test

CPSD-SL-31055-MTHD Per care label

Prints/Stamps/HTL, etc. Evaluate and record comments after 10 and 20 wash/dry cycles or 5 dry clean cycles Color Change: Grade 4.0, Self-Staining: Grade 4.5 Appearance: No cracking, peeling, distortion, color transfer, etc. Text must be legible

Page 56: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 56 of 72 February 2020 Version 5

802 Special Claims Page 3 of 3

TEST CITATION / METHOD CRITERIA

*Thermal transmittance of textile materials

ASTM D1518 If Claimed Report result or verify claim (1 rep) 0.6 CLO

*Ultra violet protection factor (UPF)

AATCC 183-2004 / ASTM D6544-00 (2007) / ASTM

D6603-10

If Claimed Perform on original and after simulated use & care (as prepared per ASTM D6544). Report UPF rating only. The UPF rating shall be given as per ASTM D6603 below: 15-24: Good UV protection 25-39: Very good UV protection 40-50+: Excellent UV protection

*Unbreakable Buttons (required for all dress shirt buttons, style # prefix is “DS”)

AATCC 150 (mod)/ ASTM D5171

If Claimed or Requested AATCC 150 (mod): Evaluate 30 buttons after 5 / 10 / 15 / 20 HL: No chips, cracks or breakage ASTM D5171: Evaluate 30 buttons under 5.5 in-oz impact energy: No chips, cracks or breakage

*Waterproof AATCC 127 option 2 or ASTM D751 option A

If Claimed Waterproof Test Original & after 5 HL or 1 DC (per care label) 2000 mm w.c. (200 cm w.c. or 196 mbar or 2.86 psi)

*Water Repellency: Spray Test

AATCC 22 If Claimed Water Repellent Test Original & after 5 HL or 1 DC (per care label) Original: ISO 90 min. / After 5 washes/1DC: ISO 70 min.

*Water Resistance: Rain Test AATCC 35

If Claimed Water Resistant Less than 1 gram Customs test on garments: no more than 1 gm of water penetration at 600 mm pressure for a 2 min duration

*Water Vapor Transmission ASTM E96 (b)

Upright Cup Method Breathable Claim Test Original & after 3 HL or 1 DC (per care label) Requirement: ≥ 500 g/m2 / 24 hours

*Water Wicking (Test All Colors)

AATCC 197

Moisture Management Claim of Wicking or Cool Dry Test Original & after 5 HL or 1 DC (per care label) 3 inches minimum at 30 minutes Pass/Fail based on after care test results only

*Wrinkle Resistance / Durable Press Evaluate after 5 HL

AATCC 124/ AATCC 143

Wrinkle Resistant/Wrinkle Free/Non Iron Claims Pre-Cure Process/Post-Cure Process Fabric Smoothness: Grade 3.5 min Seams/Pleats (pants)/Creases (pants): Grade 3.5 min

Easy Care Claims Fabric Smoothness: Grade 3 min Seams/Pleats (pants)/Creases (pants): Grade 3 min

Seams include: collar, yoke, shoulder, armhole, cuff, sleeve, front placket, side seam, pocket, fly closure, inseam, seat

Page 57: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 57 of 72 February 2020 Version 5

803 Belts (sold separately) Note: See protocol 805 for Belts sold together with a garment

Page 1 of 3

TEST CITATION / METHOD CRITERIA

Labeling

Uniform Packaging and Labeling Regulations (Applicable to the Packaging Materials)

NIST Uniform Laws and Regulations Handbook 130

Manufacturer, Packer, or Distributor’s Name & Address (City, State & Zip).

Product Identification

Net quantity of contents shall be expressed in terms of weight or mass, measure, numerical count, or combination so as to give accurate information to facilitate consumer comparison (U.S. and metric units).

Country of Origin Marking 19 CFR 134

Shall indicate country of origin legibly, permanently, and in comparable size and close proximity to any mention of country other than country in which the article was manufactured or produced. Must be visible at point of purchase.

Leather Labeling / Imitation Leather (Verify label claims)

FTC / 16 CFR 24

Must conform to guidelines for leather content labeling. If all or part of a product is made of non-leather material that appears to be leather, the non-leather material must be disclosed on the retail packaging. The disclosure must be of such conspicuousness and clarity as to be noted by consumers casually inspecting the product. The disclosure must be in close proximity to the product identification.

Fiber Content (Verify label claims) 16 CFR 303 / 16 CFR 300

Must Comply to the Label (Belts are exempt unless something is stated about fiber content or it contains wool)

RN# Or WPL # Or Mfr. Name 16 CFR 303 / 16 CFR 300

If listed, report actual (Belts are exempt unless something is stated about fiber content or it contains wool)

Claim verification CPSD-HL-1004 Must Comply with All Claims

Page 58: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 58 of 72 February 2020 Version 5

803 Belts (sold separately) Note: See protocol 805 for Belts sold together with a garment

Page 2 of 3

TEST CITATION / METHOD CRITERIA

Analytical

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

Flammability

*Flammability Of Clothing Textiles (as applicable)

16 CFR 1610 Class 1 Belts less than 2 inches wide are not required to be tested

*Flammability of Vinyl Plastic Film (as applicable)

16 CFR 1611 Must Comply With Regulation Belts less than 3 inches wide are not required to be tested

Physical Characteristics

Dimensions CPSD-HL-01056-MTHD

(Standard Measurement) Total Length, Total Width

Number of Holes CPSD-HL-01056-MTHD

(Standard Measurement) Report actual

Sharp Point/ Edges 16 CFR 1500.48/ 1500.49

(Modified to test on Adult items)

Shall Have No Sharp Points/ Edges, Other Than Those Required For Function

Defects / Workmanship CPSD-HL-01057-MTHD

(Visual)

Shall have no components missing, malformed and / or fractured and no discernible surface degradation, including crazing, shivering, bubbles, cracks, chips, scratches, scuff marks, blisters, etc.

Page 59: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 59 of 72 February 2020 Version 5

803 Belts (sold separately) Note: See protocol 805 for Belts sold together with a garment

Page 3 of 3

TEST CITATION / METHOD CRITERIA

Performance

Effects Of Extreme Temperature CPSD-HL-01012-MTHD No noticeable change after 24 Hours @ 0°F and 140°F

Functionality CPSD-GB-01058-MTHD Shall function as intended

Effects of Humidity CPSD-HL-01007-MTHD No noticeable change after 48 hours @ 95% RH @ 95°F

Buckle Strength/Buckle Durability

Actual Use No failure after 500 cycles of operation

Buckle/Strap Strength Not applicable to military style belts, as shown below:

ASTM D5034-95 80 lbs./in. minimum

Belt hole rupture resistance ASTM D5034 mod 20 lbs. minimum

Bonding Strength CPSD-SL-81003-MTHD 15 lbs./4 inches

Tensile Strength ASTM D5034 mod 40 lbs. minimum

Belt Loop Attachment ASTM D5034 mod 15 lbs. minimum

Stitch Reinforcement Strength CPSD-SL-81005-MTHD 35 lbs. minimum (Functional)

Flexing CPSD-SL-81002-MTHD 25,000 cycles minimum

Buckle / Clasp Functionality Actual Use No fractures / breakage of buckle / clasp

Resistance To Corrosion (All Metal Components)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Colorfastness

CF to Crocking (face & back) AATCC 8/116 Vinyl/Textile: Dry: Grade 4 minimum Wet: Grade 3 minimum

Leather/Suede: Dry: Grade 3.5 minimum Wet: Grade 2.5 minimum

CF to Perspiration AATCC 15 (mod) Back side of belt at the front area: Grade3.0 minimum Buckle: No discoloration or degradation of surface finish/color

Page 60: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 60 of 72 February 2020 Version 5

804 Suspenders Page 1 of 2

TEST CITATION / METHOD CRITERIA

Labeling

Uniform Packaging and Labeling Regulations (Applicable to the Packaging Materials)

NIST Uniform Laws and Regulations Handbook 130

Manufacturer, Packer, or Distributor’s Name & Address (City, State & Zip).

Product Identification

Net quantity of contents shall be expressed in terms of weight or mass, measure, numerical count, or combination so as to give accurate information to facilitate consumer comparison (U.S. and metric units).

Country of Origin Marking 19 CFR 134

Shall indicate country of origin legibly, permanently, and in comparable size and close proximity to any mention of country other than country in which the article was manufactured or produced. Must be visible at point of purchase.

RN# Or WPL # Or Manufacturer Name

16 CFR 303 / 16 CFR 300

If listed, report actual. (Suspenders are exempt unless something is stated about fiber)

Fiber Content (Verify if claimed) Do not test if not claimed

16 CFR 303 / 16 CFR 300

Must Comply to the Label (Suspenders are exempt unless something is stated about fiber)

Claim verification CPSD-GB-08612-MTHD Must comply with all claims and conduct additional testing as needed

Analytical

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

Flammability

*Flammability Of Clothing Textiles (as applicable)

16 CFR 1610 Class 1 Suspenders less than 2 inches wide are not required to be tested

*Flammability of Vinyl Plastic Film (as applicable)

16 CFR 1611 Must Comply With Regulation Suspenders less than 3 inches wide are not required to be tested

Page 61: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 61 of 72 February 2020 Version 5

804 Suspenders Page 2 of 2

TEST CITATION / METHOD CRITERIA

Physical Characteristics

Total Length CPSD-HL-01056-MTHD

(Standard Measurement) Tape measure end to end

Sharp Point/ Edges 16 CFR 1500.48/ 1500.49

(Modified to test on Adult items)

Shall Have No Sharp Points/ Edges, Other Than Those Required For Function

Defects / Workmanship CPSD-HL-01057-MTHD

(Visual)

Shall have no components missing, malformed and / or fractured and no discernible surface degradation, including crazing, shivering, bubbles, cracks, chips, scratches, scuff marks, blisters, etc.

Performance

Functionality CPSD-GB-01058-MTHD Shall function as intended.

Effects Of Extreme Temperature

CPSD-HL-01012-MTHD No noticeable change @ 24 Hours at 0°F and 140°F

Effects of Humidity CPSD-HL-01007-MTHD No noticeable change after 48 hours @ 95% RH @ 95°F

Tension & Elongation (Elastic Only)

ASTM D4964 Calculate 90% (min) recovery when stretch to max or over 100% of original length

Stitch/Seam Reinforcement Strength

ASTM D 1683 (Mod) 100 lbs. / in. (min.)

Clip/Leather Ears attachment strength

ASTM D5034 mod. 75 lbs./in. (min.)

Clip Durability Actual Use Shall have no failure or loss in serviceability after 500 cycles (Open/close or Clip/unclip)

Clip performance strength ASTM D5034 mod Shall be able to clip and hold onto a 2 layer of 8 oz./sq. yd. woven fabric when 13 lbs. of force is applied

Resistance To Corrosion (All Metal Components)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Colorfastness

CF to Crocking (Face & Back) AATCC 8/116 Vinyl/Textile: Dry: Grade 4/Wet: Grade 3 minimum Leather/Suede: Dry: Grade 3.5/Wet: Grade 2.5 minimum

CF to Perspiration AATCC 15 Back side of suspenders: Grade3.0 minimum Metal Hardware: No discoloration or degradation of surface finish/color

Page 62: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 62 of 72 February 2020 Version 5

805 Belts (sold together with a garment)

Page 1 of 1

TEST CITATION / METHOD CRITERIA

Analytical

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

Flammability

*Flammability Of Clothing Textiles (as applicable)

16 CFR 1610 Class 1 Belts less than 2 inches wide are not required to be tested

*Flammability of Vinyl Plastic Film (as applicable)

16 CFR 1611 Must Comply With Regulation Belts less than 3 inches wide are not required to be tested

Physical Characteristics

Dimensions CPSD-HL-01056-MTHD

(Standard Measurement) Total Length, Total Width

Manufacturing Defects / Workmanship

CPSD-HL-01057-MTHD (Visual)

No major defects. Shall have no components missing, malformed, and /or fractured, Shall demonstrate good/ even construction, with no sharp edges, sharp points or discoloration.

Performance

Buckle/Strap Attachment Strength

ASTM D5034 mod 40 lbs./in Minimum

Tensile Strength ASTM D5034 mod 40 lbs. Minimum

Resistance To Corrosion (All Metal Components)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails.

Colorfastness

CF to Crocking AATCC 8/116 Textile: Dry: Grade 4/Wet: Grade 3 minimum Leather/Suede: Dry: Grade 3.5/Wet: Grade 2.5 minimum

CF to Perspiration AATCC 15 Grade3.0 minimum

Page 63: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 63 of 72 February 2020 Version 5

806 Accessories (Scarves, Neck Warmers, Gloves, Handkerchiefs, Earmuffs) Page 1 of 2

TEST CITATION / METHOD CRITERIA

Analytical

*California Proposition 65 (as applicable per Adult item)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH Value AATCC 81 5-9

Labeling

Country of Origin Marking 19 CFR 134/Visual As Applicable per Regulations

Fiber Content / Leather Labeling

16 CFR 303/300, FTC / 16 CFR 24/Visual

As Applicable per Regulations

RN# Or WPL # Or Mfr. Name 16 CFR 303/300/Visual As Applicable per Regulations

Care Label 16 CFR 423/Visual As Applicable per Regulations (not required for gloves, handkerchiefs and earmuffs)

Size Visual As Applicable per Regulations

Flammability

*Flammability Of Clothing Textiles (as applicable)

16 CFR 1610 Class 1

Physical Characteristics

*Fiber Analysis (if claimed or required per regulations)

AATCC 20/20A 0% Single Fiber ± 3% Blends

Dimensions CPSD-HL-01056-MTHD

(Standard Measurement) Total Length, Total Width

Manufacturing Defects / Workmanship

CPSD-HL-01057-MTHD (Visual)

No major defects. Shall have no components missing, malformed, and /or fractured, Shall demonstrate good/ even construction, with no sharp edges, sharp points or discoloration.

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 150 Per Care Instructions

Shrinkage: -5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, damaged components, open seams, noticeable puckering, etc. Pilling: Grade4.0 Color Change: Grade4.0 Self-Staining: Grade4.5

Seam Skew/Torque AATCC TS-004 5% maximum

Page 64: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 64 of 72 February 2020 Version 5

806 Accessories (Scarves, Neck Warmers, Gloves, Handkerchiefs, Earmuffs) Page 2 of 2

Notes: 1. Any components not previously tested are required to test to appropriate standard. 2. Please refer to special claims protocol as applicable.

Attachment Strength

Pull Test

15 lbs./10 Seconds

Component Functionality Function as Intended

Resistance To Corrosion (All Metal Components)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components - indicate pass or fail for each piece/section, and include before and after pictures of each piece/section that Fails

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Dry-cleaning AATCC 158 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Non-Chlorine Bleach AATCC TS-001 With Suppressor for pastels only Grade4.0

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

CF to Light AATCC 16, Option 3 Provide ratings after 10 & 20 AFU Pass/Fail based on 20 AFU rating only Grade 3.0 @ 20 AFU

CF to Water AATCC 107 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

TEST CITATION / METHOD CRITERIA

Performance (continued)

Page 65: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 65 of 72 February 2020 Version 5

807 Rain Poncho

Page 1 of 2

TEST CITATION / METHOD CRITERIA Labeling

Textile Fiber Products Identification Act Care Labeling Rule

Visual

Fiber Content Label RN# Country of Origin Care Label Size

Uniform Packaging and Labeling Regulations

NIST Uniform Laws and Regulations Handbook

130

Manufacturer, Packer, or Distributor’s Name & Address (City, State & Zip) Product Identification Shall indicate country of origin legibly, permanently, and in comparable size and close proximity to any mention of country other than country in which the article was manufactured or produced. Must be visible at point of purchase.

Claim verification - level 2 CPSD-GB-08612-MTHD MUST CONTACT DXL GROUP BEFORE ANY ADDITIONAL CLAIM TESTING IS CONDUCTED. Examine the retail packaging (or submitted artwork). Record each objective (factual) claim which can be substantiated by the testing within the protocols and rate accordingly. Record testing that extends beyond existing net quantity / dimensional testing on this protocol. Record all other objective (factual) and subjective (opinion) claims as “NT” and rate as “DATA”. Record information evaluated between the graphic imagery and the product. Record disclaimers on datasheet.

Analytical

*California Proposition 65 (Do not test non-accessible parts)

CPSD-AN-PTCL-06572-US Tested against the ADULT requirements of California Proposition 65 as applicable

*Lead in surface coating (As applicable-DO NOT test textile fabric or garment labels)

CPSC-CH-E1003-09.1 / AOAC 974.02 (mod.)

Shall not exceed 90 ppm (0.009% by weight)

*Lead in substrate (as applicable)

CPSD-AN-00185-MTHD / CPSD-AN-00196-MTHD

Shall not exceed 100 ppm (0.01% by weight)

Page 66: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 66 of 72 February 2020 Version 5

807 Rain Poncho Page 2 of 2

TEST CITATION / METHOD CRITERIA Analytical (continued)

Formaldehyde Spot Test (Applicable to areas of direct skin contact)

In-house test method / CPSD-AN-00018-

MTHD

Negative (Only test fabric that has direct skin contact) If positive continue to Quantitative. If inconclusive do NOT proceed to Quantitative.

*Formaldehyde Quantitative EN ISO 14184-1:2011 <75 ppm

Flammability

Flammability Of Clothing Textiles (as Applicable)

16 CFR 1610 Class 1 (if not exempt) - All Colors

*Flammability of Vinyl Plastic Film(If Applicable)

16 CFR 1611 Must Comply With Regulation

Physical Characteristics

*Material Identification AATCC 20 FTIR Analysis

Material Weight ASTM D3776-09 -5%/+10% from claim

Thickness (mm) CPSD-HL-01056-MTHD Report actual

Defects/Workmanship Visual Report all defects

Performance

Non-Pocket Stress Points ASTM D1683-2011

(Mod.) 15 lbs.

Unsnapping Force (Must be tested on garment or attached to a mock up panel)

CPSD-SL-31045-MTHD Maximum 8 lbs. Fails if the snap is detached from the garment during the test

Holding Strength (Must be tested on garment or attached to a mock up panel)

ASTM D7142 15 lbs./10 seconds

Water Resistance : Rain Test AATCC 35 Less than 1 gram

*Resistance To Corrosion (Metal only)

ASTM B117 (Modified=1% salt (fog)

spray)

Shall withstand 24 hours in 1% salt spray (fog) with no noticeable oxidation/corrosion/visual changes. Test all applicable components.

Colorfastness

CF to Crocking AATCC 8/116 Dry Class 4.0 Wet Class 3.0

CF to Water AATCC 107 Color Change: Grade4.0 Staining: Grade3.5

Page 67: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 67 of 72 February 2020 Version 5

808 Rib Cuffs /Collars /Bottom Hems /Bottom Bands Page 1 of 1

TEST CITATION / METHOD CRITERIA Analytical

*AZO Dyes (submitter must provide OEKO-TEX certificate)

EN 14362-1:2012 / ISO 17234-1:2010

<30 mg/kg (AZO test is invoiced to the submitter if they do not provide an OEKO-TEX certificate)

pH Value AATCC 81 5-9

Performance

Dimensional Stability-Home Laundering (3 washes)

AATCC 135 Per Care Instructions

-5% Growth: +2%

Dimensional Stability-Dry-cleaning (1 cycle)

AATCC 158 Per Care Instructions

Shrinkage: -2% Growth: +1%

General Appearance after care (3HL or 1 DC)

Visual CPSD-SL-31055-MTHD

No distortion, defects, excessive puckering, etc. Color Change: Grade 4.0 Pilling: Grade 4.0

Colorfastness

CF to Home Laundering AATCC 135 (modified) Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Crocking AATCC 8/116 Dry Grade4.0 Wet Grade3.0

CF to Water AATCC 107 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

CF to Perspiration AATCC 15 Color Change: Grade4.0 Staining: Grade3.5 Self-Staining: Grade4.5

Stretch & Recovery ASTM D2594 Recovery: 85% minimum Growth: 5% maximum ( Measure after 30 and 60 minutes)

Page 68: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 68 of 72 February 2020 Version 5

809 Premium Pants - Additional Performance Tests

Page 1 of 1

TEST CITATION / METHOD CRITERIA Performance

*Water Repellency: Spray Test (Test all colors)

AATCC 22 Test Original & after 5 HL or 1 DC (per care label) Original: ISO 90 minimum After 5 washes/1DC: ISO 70 minimum

*Anti-Fade (Test all colors)

CPSD-SL-31055-MTHD Evaluate after 5 / 10 / 15 / 20 washes Color Change: Grade 4.0 minimum

*Soil Release: Oily Stain Method (Test all colors)

AATCC 130 Test Original & after 5 HL or 1 DC (per care label) Original: Grade 3.5 After 5 washes/1DC: Grade 3.0

*Wrinkle Resistance / Durable Press (Test all colors)

AATCC 143 Evaluate after 5 HL Fabric Smoothness: Grade 4 min. Seams/Pleats/Creases: Grade 4 min.

Page 69: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 69 of 72 February 2020 Version 5

Zipper Requirements Page 1 of 4

Fastener Class (Chain Width: inch)

1-2 (0.125-0.180)

Zipper Item Chain Width: inch)

0.169 0.169 0.163 0.193

Brass Aluminum CEF CEF

kgf N lbs. kgf N lbs. kgf N lbs. kgf N lbs. Chain Crosswise Strength 35.0 343.0 77.2 25.0 245.0 55.1 35.0 343.0 77.2 40.0 392.0 88.2 Separating Unit Crosswise Strength

9.0 88.2 19.8 9.0 88.2 19.8 - - - - - -

Element Pull Off Strength 3.5 34.3 7.7 2.4 23.5 5.3 - - - - - - Element Slippage Strength 2.7 26.5 6.0 2.4 23.5 5.3 - - - - - - Slider Lock Holding Strength

4.0 39.2 8.8 3.3 37.2 8.4 2.0 19.6 4.4 2.5 24.5 5.5

Tab Pull Off (90°) 15.0 147.0 33.1 15.0 147.0 33.1 8.0 78.4 17.6 8.0 78.4 17.6 Tab Twist Off 3.0 29.4 2.6 3.0 29.4 2.6 1.5 14.7 1.3 1.5 14.7 1.3 Operability (open/close) 0.30 2.94 0.66 0.30 2.94 0.66 0.50 4.90 1.10 0.50 4.90 1.10 Top Stop Holding Strength 7.0 68.6 15.4 7.0 68.6 15.4 7.0 68.6 15.4 9.0 88.2 19.8 Bottom Stop Holding, Stringer Separation Plastic Bottom

5.0 49.0 11.0 4.5 44.1 9.9 3.0 29.4 6.6 3.5 34.3 7.7

Slider Type DA DA DA DA

Fastener Class (Chain Width: inch)

3-4 (0.125-0.180)

Zipper Item Chain Width: inch)

0.177 0.177 0.185 0.163

Brass Aluminum Plastic CEF

kgf N lbs. kgf N lbs. kgf N lbs. kgf N lbs. Chain Crosswise Strength 55.0 539.0 121.3 35.0 343.0 77.2 27.0 264.6 59.5 40.0 392.0 88.2 Separating Unit Crosswise Strength

9.0 88.2 19.8 9.0 88.2 19.8 9.0 88.2 19.8 6.0 58.8 13.2

Element Pull Off Strength 6.0 58.8 13.2 3.5 34.3 7.7 2.5 24.5 5.5 - - - Element Slippage Strength 4.5 44.1 9.9 2.7 26.5 6.0 3.5 34.3 7.7 - - - Slider Lock Holding Strength 9.0 88.2 19.8 4.0 39.2 8.8 3.0 29.4 6.6 2.0 19.6 4.4 Tab Pull Off (90°) 18.0 176.4 39.7 15.0 147.0 33.1 12.0 117.6 26.5 8.0 78.4 17.6 Tab Twist Off 4.6 45.1 4.0 3.0 29.4 2.6 3.0 29.4 2.6 2.0 19.6 1.7 Operability (open/close) 0.35 3.43 0.77 0.35 3.43 0.77 0.50 4.90 1.10 0.40 3.92 0.88 Top Stop Holding Strength 9.0 88.2 19.8 8.0 78.4 17.6 8.0 78.4 17.6 8.0 78.4 17.6 Bottom Stop Holding, Stringer Separation Plastic Bottom

8.0 78.4 17.6 6.0 58.8 13.2 5.0 49.0 11.0 7.0

5.0

68.6

49.0

15.4

11.0 Slider Type GS DA DA DA

Page 70: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 70 of 72 February 2020 Version 5

Zipper Requirements Page 2 of 4

Fastener Class (Chain Width: inch)

5-7 (A) (0.180-0.310)

Zipper Item Chain Width: inch)

0.197 0.226 0.226 0.226

Brass Brass Brass Aluminum

kgf N lbs. kgf N lbs. kgf N lbs. kgf N lbs. Chain Crosswise Strength

60.0 588.0 132.3 65.0 637.0 143.3 50.0 490.0 110.3 50.0 490.0 110.3

Separating Unit Crosswise Strength

10.0 98.0 22.1 12.0 117.6 26.5 12.0 117.6 26.5 12.0 117.6 26.5

Element Pull Off Strength

7.5 73.5 16.5 9.0 88.2 19.8 6.0 58.8 13.2 6.0 58.8 13.2

Element Slippage Strength

4.5 44.1 9.9 5.0 49.0 11.0 4.5 44.1 9.9 4.0 39.2 8.8

Slider Lock Holding Strength

10.0 98.0 22.1 11.0 107.8 24.3 6.0 58.8 13.2 6.0 58.8 13.2

Tab Pull Off (90°) 20.0 196.0 44.1 25.0 245.0 55.1 18.0 176.4 39.7 18.0 176.4 39.7 Tab Twist Off 4.6 45.1 4.0 5.0 49.0 4.3 5.0 49.0 4.3 5.0 49.0 4.3 Operability (open/close)

0.45 4.41 0.99 0.50 4.90 1.10 0.50 4.90 1.10 0.40 3.92 0.88

Top Stop Holding Strength

10.0 98.0 22.1 11.0 107.8 24.3 10.0 98.8 22.1 10.0 98.0 22.1

Bottom Stop Holding, Stringer Separation Plastic Bottom

9.0 88.2 19.8 11.0 107.8 24.3 8.0 78.4 17.6 9.0 88.2 19.8

Slider Type GS GS DA DA

Fastener Class (Chain Width: inch)

5-7 (A) (0.180-0.310)

Zipper Item Chain Width: inch)

0.224 0.203 0.203 0.256

Plastic Plastic CEF CEF

kgf N lbs. kgf N lbs. kgf N lbs. kgf N lbs. Chain Crosswise Strength

40.0 392.0 88.2 32.0 313.6 70.6 55.0 539.0 121.3 65.0 637.0 143.3

Separating Unit Crosswise Strength

12.0 117.6 26.5 11.0 107.8 24.3 6.0 78.4 17.6 12.0 117.6 26.5

Element Pull Off Strength

5.0 49.0 11.0 3.5 34.3 7.7 - - - - - -

Element Slippage Strength

5.0 49.0 11.0 4.0 39.2 8.8 - - - - - -

Slider Lock Holding Strength

3.5 34.3 7.7 4.0 39.2 8.8 3.0 29.4 6.6 5.0 49.0 11.0

Tab Pull Off (90°) 18.0 176.4 39.7 15.0 147.0 33.1 18.0 176.4 39.7 25.0 245.0 55.1 Tab Twist Off 5.0 49.0 4.3 4.0 39.2 3.5 4.5 44.1 3.9 5.0 49.0 4.3 Operability (open/close)

0.70 6.86 1.54 0.70 6.86 1.54 0.50 4.90 1.10 0.70 6.86 1.54

Top Stop Holding Strength

10.0 98.0 22.1 9.0 88.2 19.8 9.0 88.2 19.8 12.0 117.6 26.6

Bottom Stop Holding, Stringer Separation Plastic Bottom

9.0 88.2 19.8 6.0 58.8 13.2 10.0

8.0

98.0

78.4

22.1

17.6

12.0

10.0

117.6

98.0

26.6

22.1 Slider Type DA DA DA DA

Page 71: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 71 of 72 February 2020 Version 5

Zipper Requirements

Page 3 of 4

Fastener Class (Chain Width: inch)

5-7 (B) (0.180-0.310)

Zipper Item Chain Width: inch)

0.252 0.252 0.283

Brass Aluminum CEF

kgf N lbs. kgf N lbs. kgf N lbs. Chain Crosswise Strength 65.0 637.0 143.3 40.0 392.0 88.2 80.0 784.0 176.4 Separating Unit Crosswise Strength 15.0 147.0 33.1 15.0 147.0 33.1 15.0 147.0 33.1 Element Pull Off Strength 8.0 78.4 17.6 5.0 49.0 11.0 - - - Element Slippage Strength 5.5 53.9 12.1 4.5 44.1 9.9 - - - Slider Lock Holding Strength 6.0 58.8 13.2 6.0 58.8 13.2 6.0 58.8 13.2 Tab Pull Off (90°) 20.0 196.0 44.1 20.0 196.0 44.1 25.0 245.0 55.1 Tab Twist Off 6.0 58.8 5.2 6.0 58.8 5.2 7.0 68.6 6.1 Operability (open/close) 0.60 5.88 1.32 0.60 5.88 1.32 0.70 6.86 1.54 Top Stop Holding Strength 13.0 127.4 28.7 13.0 127.4 28.7 13.0 127.4 28.7 Bottom Stop Holding, Stringer Separation Plastic Bottom

10.0 98.0 22.1 10.0 98.0 22.1 14.0 137.2 30.9

Slider Type DA DA DA

Fastener Class (Chain Width: inch)

5.7 (B) (0.180 – 0.310)

8.9 (0.310-0.390)

Zipper Item Chain Width: inch)

0.291 0.291 0.291

Brass Aluminum Plastic

kgf N lbs. kgf N lbs. kgf N lbs. Chain Crosswise Strength 65.0 637.0 143.3 40.0 392.0 88.2 50.0 490.0 110.3 Separating Unit Crosswise Strength 15.0 147.0 33.1 15.0 147.0 33.1 17.0 166.6 37.5 Element Pull Off Strength 8.5 83.3 18.7 5.5 53.9 12.1 8.0 78.4 17.6 Element Slippage Strength 6.0 58.8 13.2 5.5 53.9 12.1 7.0 68.6 15.4 Slider Lock Holding Strength 7.0 68.6 15.4 7.0 68.6 15.4 6.0 58.8 13.2 Tab Pull Off (90°) 25.0 245.0 55.1 25.0 245.0 55.1 20.0 196.0 44.1 Tab Twist Off 7.0 68.6 6.1 7.0 68.6 6.1 7.0 68.6 6.1 Operability (open/close) 0.70 6.86 1.54 0.70 6.86 1.54 0.70 6.86 1.54 Top Stop Holding Strength 15.0 147.0 33.1 15.0 147.0 33.1 15.0 147.0 33.1 Bottom Stop Holding, Stringer Separation Plastic Bottom

12.0 117.6 26.5 12.0 117.6 26.5 14.0 137.2 30.9

Slider Type DA DA DA

Page 72: DXL Group QUALITY ASSURANCE TEST MANUAL · 2020-02-25 · Include the trf, the supplier’s OEKO-TEX certificate and the test items with all BV test submissions. ... The final test

Page 72 of 72 February 2020 Version 5

Zipper Requirements Page 4 of 4

Fastener Class (Chain Width: inch)

10 (0.320-0.500)

Zipper Item Chain Width: inch)

0.335 0.335 0.346 0.425

Brass Aluminum Plastic CEF

kgf N lbs. kgf N lbs. kgf N lbs. kgf N lbs. Chain Crosswise Strength 80.0 784.0 176.4 50.0 490.0 110.3 60.0 588.0 132.3 100.0 980.0 220.5 Separating Unit Crosswise Strength

22.0 215.6 48.5 22.0 215.6 48.5 22.0 215.6 48.5 22.0 215.6 48.5

Element Pull Off Strength 11.0 107.8 24.3 7.5 73.5 16.5 9.0 88.2 19.8 - - - Element Slippage Strength 8.5 83.3 18.7 7.5 73.5 16.5 10.0 98.0 22.1 - - - Slider Lock Holding Strength

7.0 68.6 15.4 7.0 68.6 15.4 7.0 68.6 15.4 7.0 68.6 15.4

Tab Pull Off (90°) 30.0 294.0 66.2 30.0 294.0 66.2 30.0 294.0 66.2 30.0 294.0 66.2 Tab Twist Off 8.0 78.4 6.9 8.0 78.4 6.9 8.0 78.4 6.9 8.0 78.4 6.9 Operability (open/close) 0.80 7.84 1.76 0.80 7.84 1.76 0.90 8.82 1.98 0.90 8.82 1.98 Top Stop Holding Strength 18.0 176.4 39.7 18.0 176.4 39.7 18.0 176.4 39.7 18.0 176.4 39.7 Bottom Stop Holding, Stringer Separation Plastic Bottom

15.0 147.0 33.1 15.0 147.0 33.1 17.0 166.6 37.5 18.0 176.4 39.7

Slider Type DA DA DA DA

Note: 1 kgf=9.8N 1 kgf=2.206 lbs. 1 cm=0.3937 inch

Methods: Chain Crosswise Strength ASTM D2061; 14.1

Separating Unit Crosswise Strength ASTM D2061; 30.3

Element Pull Off Strength ASTM D2061; 14.2

Element Slippage Strength ASTM D2061; 14.3

Slider Lock Holding Strength ASTM D2061; 87.1

Tab Pull Off (90°) ASTM D2061; 68.1

Tab Twist Off ASTM D2061; 52.1

Operability (open/close) ASTM D2062; 16

Top Stop Holding Strength ASTM D2061; 22.2

Bottom Stop Holding, Stringer Separation ASTM D2061; 22.5