Astrup MDS Versjon nr: 1.2 Dato opprettet: 2013-04-05 Forfatter: LN Revider av: DBF Sist oppdatert: 2014-01-13 KVALITET, MANGFOLD OG GODT SAMARBEID 1 1.4418 QT900 Astrup MDS 1.4418 QT900 Material Description Quality Hot rolled/ forged stainless bar steel Grinded, stainless bars steel Hardened and tempered EN 1.4418 / S165M / SS 2387 QT 900 Chemical composition C % Si % Mn % Cr % Mo % Ni % P % S % N % 0,02 0,05 0,3 0,7 0,6 1,0 15,0 17,0 0,8 1,25 4,5 5,5 ≤0,04 0,005 0,015 0,02 0,015 Mechanical properties Yield strength Tensile strength Elongation Contraction Impact Value Hardness Hardness Rp 0,2 % /N/mm 2 ) Rm (N/mm 2 ) A5 % Z % Kv/J (-40 0 C) HRC HB Min 750 Min 900 Min 16 Min 40 Min 32 Min 280 Max 1100 Max 340 Technical requirements EN 10088-3 QT900 X4CrNiMo 16-5-1 Heat treatment: Hardening at 1000º C / cooled in air followed by tempering at 580-640º C / cooled in air. UT-testing ≥ 25mm acc. to EN 10308 type 1a, tab.2, class 4. Certificate Acc to EN 10204/3.1 Form of supply Lengths from 3-7 meter, depending on diameter. Max weight per subject: 5000 kg Marking Astrup purchase number. Eeach bar to be marked or hard stamped with charge number, quality and dimension.

Astrup

Embed Size (px)

DESCRIPTION

Astrup

Citation preview

  • Astrup MDS Versjon nr: 1.2 Dato opprettet: 2013-04-05 Forfatter: LN Revider av: DBF Sist oppdatert: 2014-01-13

    1. Feltutfylling K V A L I T E T , M A N G F O L D O G G O D T S A M A R B E I D

    1

    1.4418 QT900

    Astrup MDS 1.4418 QT900

    Material Description Quality

    Hot rolled/ forged stainless bar steel Grinded, stainless bars steelHardened and tempered

    EN 1.4418 / S165M / SS 2387QT 900

    Chemical composition

    C % Si % Mn % Cr % Mo % Ni % P % S % N %

    0,02 0,05

    0,3 0,7

    0,6 1,0

    15,0 17,0

    0,8 1,25

    4,5 5,5

    0,04

    0,005 0,015

    0,02 0,015

    Mechanical propertiesYield strength Tensile strength Elongation Contraction Impact Value Hardness Hardness Rp 0,2 % /N/mm2) Rm (N/mm2) A5 % Z % Kv/J (-40 0C) HRC HBMin 750 Min 900 Min 16 Min 40 Min 32 Min 280

    Max 1100 Max 340

    Technical requirements

    EN 10088-3 QT900X4CrNiMo 16-5-1 Heat treatment: Hardening at 1000 C / cooled in air followed by tempering at 580-640 C / cooled in air. UT-testing 25mm acc. to EN 10308 type 1a, tab.2, class 4.

    Certificate

    Acc to EN 10204/3.1

    Form of supply

    Lengths from 3-7 meter, depending on diameter. Max weight per subject: 5000 kg

    Marking

    Astrup purchase number.Eeach bar to be marked or hard stamped with charge number, quality and dimension.