Comparison with conventional Floor VS Fibermesh floor.xls

Embed Size (px)

Citation preview

  • Comparision with Conventional floor

    Sr Description Conventional Floor FIBERMESH FLOOR Significance

    1

    2 Cover block Not required Saving in time and cost

    3 Inspection

    4 Conecrete pouring

    5 Screed vibrator Same Same6 Troweling Same Same7 VDC (Varies) Same Same 8 Tensile strength 415-500 N/mm ^2 Min 1050 N/MM^2

    9 Network 12mtrs per Mtr Square Min 360 Mtr per Square Meter

    10 Reinforcment At Particular Level Throughout the section

    11 Failure mode Brittle Ductile

    Reinforcment Laying and tying

    200-250 Kg per day with 2 Bar benders 2 Helpers ( 10 hrs) for lesser diameter else varies

    One/Two person at the batching plant or at the mixer. Cutting bags and dosing

    Saving in time and labour gives early handover and cost saving

    1 no of 50 mm thick Required per sqmInspection required after reinforcement laying

    No inspection required Dramix Fibers mix homogenously in concrete due to gluing technlogy

    Work can be done with minimum supervision. Dramix fibers are engineered to suit your local needs

    Truck mixer or bag mixer has to be loacted beyond the flooring area

    Mixer can go to pouring site as there is no reinforcement

    Saving in lead time as distance between mixer and actual site is reduced

    Higher tensile strength higher crack control

    More the netwrok better the performance

    Throughout reinforcment gives excellent crack control and redistribution of loads

    Better post carck behaviour better post crack strength Ftcm