MANUFACTURED SAMPLES FOR EVALUATION AND VALIDATION OF THz

MANUFACTURED SAMPLES

CALIBRATION SAMPLES(evaluate)

BLIND SAMPLES(validate)

GLASS FIBER

CARBON FIBER

GLASS FIBER

CARBON FIBER

Impact damageOdd material inclusionDelaminationsDebondingsWater inclusion

Impact damage

Miscoating defects

Real delaminationsReal porosityReal debonding

Page 3: Barcelona, 27 th June 2013 -1- 2 nd ITFG Workshop Samples

Barcelona, 27th June 2013 -3-

2nd ITFG Workshop

STRUCTURES OF THE SAMPLES

SOLID LAMINATE

A-SANDWICH

C-SANDWICH

Page 4: Barcelona, 27 th June 2013 -1- 2 nd ITFG Workshop Samples

Barcelona, 27th June 2013 -4-

2nd ITFG Workshop

SUMMARY OF SAMPLES

CALIBRATION SAMPLES

IMPACT DAMAGE

WATER INCLUSION TEFLONS STUCKS PAPER

SHEETS

CARBON FIBER SOLID LAMINATE GLASS FIBER SOLID LAMINATE

A- SANDWICH ROHACELL A- SANDWICH HONEYCOMB C- SANDWICH ROHACELL C- SANDWICH HONEYCOMB

Page 5: Barcelona, 27 th June 2013 -1- 2 nd ITFG Workshop Samples

Barcelona, 27th June 2013 -5-

2nd ITFG Workshop

SUMMARY OF SAMPLES

BLIND SAMPLES

COATING MISPROCESS DEBONDING DELAMINATION POROSITY

CARBON FIBER SOLID LAMINATE GLASS FIBER SOLID LAMINATE

A- SANDWICH ROHACELL A- SANDWICH HONEYCOMB C- SANDWICH HONEYCOMB